Suppr超能文献

椅旁制作全瓷冠修复单颗牙:15 年临床效果观察

Long-term survival of monolithic tooth-supported lithium disilicate crowns fabricated using a chairside approach: 15-year results.

机构信息

Department of Dental Prosthetics, University Hospital Regensburg, Franz-Josef-Strauß-Allee 11, 93053, Regensburg, Germany.

Department of Prosthodontics and Materials Science, University of Leipzig, Liebigstr. 12, 04103, Leipzig, Germany.

出版信息

Clin Oral Investig. 2023 Jul;27(7):3983-3989. doi: 10.1007/s00784-023-05023-0. Epub 2023 Apr 21.

Abstract

OBJECTIVES

To investigate the clinical performance of chairside fabricated tooth-supported posterior single crowns from lithium disilicate ceramic.

MATERIALS AND METHODS

Thirty-four crowns (IPS e.max CAD, Ivoclar Vivadent, Schaan, Liechtenstein) were inserted between 2006 and 2007 and again evaluated after 15 years. Survival and success rates were calculated according to Kaplan-Meier, and the quality of the crowns was evaluated by using modified United States Public Health (USPHS) criteria.

RESULTS

Twenty-two crowns were available for recall; six patients were defined as dropouts. The mean observation period was 15.2 years (± 0.2). Six failures occurred (1 technical/5 biological) resulting in a survival rate of 80.1%. The success rate was 64.2%. The roughness of the crowns increased (p = 0.021) and the majority of adhesive gaps were discolored (p = 0.001) in comparison to baseline. The color, tooth, and crown integrity remained stable over the follow-up period (p ≥ 0.317).

CONCLUSION

The fabrication of tooth-supported lithium disilicate crowns using a chairside approach yielded acceptable long-term survival and success rates. Due to discoloration, the long-term use of dual-cure self-adhesive resin cements might result in unpleasing esthetic results.

CLINICAL RELEVANCE

The performance of posterior lithium disilicate single crowns revealed excellent to good clinical quality and an acceptable number of events after 15 years of clinical service.

摘要

目的

研究椅旁制作的硅酸锂瓷牙支持的后牙单冠的临床性能。

材料和方法

2006 年至 2007 年间共植入 34 个牙冠(IPS e.max CAD,Ivoclar Vivadent,沙安,列支敦士登),并在 15 年后再次评估。根据 Kaplan-Meier 计算生存率和成功率,并使用改良的美国公共卫生(USPHS)标准评估牙冠的质量。

结果

22 个牙冠可召回,6 名患者被定义为失访。平均观察期为 15.2 年(±0.2)。发生 6 次失败(1 次技术/5 次生物学),生存率为 80.1%。成功率为 64.2%。与基线相比,牙冠的粗糙度增加(p=0.021),并且大多数粘结间隙变色(p=0.001)。颜色、牙齿和牙冠完整性在随访期间保持稳定(p≥0.317)。

结论

使用椅旁方法制作的牙支持硅酸锂瓷冠具有可接受的长期生存率和成功率。由于变色,长期使用双固化自粘结树脂水门汀可能会导致不美观的美学效果。

临床相关性

后牙硅酸锂单冠的性能在 15 年的临床服务后显示出良好的临床质量和可接受的事件数量。

https://cdn.ncbi.nlm.nih.gov/pmc/blobs/7898/10329614/28b4bbeb8528/784_2023_5023_Fig1_HTML.jpg

文献AI研究员

20分钟写一篇综述,助力文献阅读效率提升50倍。

立即体验

用中文搜PubMed

大模型驱动的PubMed中文搜索引擎

马上搜索

文档翻译

学术文献翻译模型,支持多种主流文档格式。

立即体验