Occupational Medicine, Finnish Institute of Occupational Health (FIOH), Helsinki, Finland.
Contact Dermatitis. 2024 Sep;91(3):212-221. doi: 10.1111/cod.14621. Epub 2024 Jul 2.
Isocyanates are used as starting materials of polyurethane (PU) products. They are relatively important occupational skin sensitizers.
To analyse results of a large isocyanate patch test series of 19 isocyanate test substances and 4,4'-diaminodiphenylmethane (MDA), a marker of 4,4'-diphenylmethane diisocyanate (MDI) hypersensitivity.
Test files were screened for positive reactions in the isocyanate series. Patients with positive reactions were analysed for occupation, exposure and diagnosis.
In 2010-2019, 53 patients had positive reactions in the series (16% of 338 patients tested). MDA, the well-established screening substance for MDI allergy, was positive in 30 patients, an in-house monomeric MDI test substance in 23 patients and 3 different polymeric MDI test substances in 19-21 patients. We diagnosed 16 cases of occupational allergic contact dermatitis (OACD) from MDI including 3 pipe reliners. Hexamethylene-1,6-diisocyanate (HDI) oligomers in paint hardeners caused 5 cases of OACD, more cases than 2,4-toluene diisocyanate (TDI; n = 3) and isophorone diisocyanate (IPDI; n = 1) put together.
In contrast to previous studies, polymeric MDI test substances were not superior to a monomeric MDI. Pipe reliners may get sensitised not only by epoxy products and acrylates but also by MDI in hardeners of PU pipe coatings. HDI oligomers were the second most important causes of OACD after MDI.
异氰酸酯是聚氨酯(PU)产品的起始原料,是相对重要的职业性皮肤致敏原。
分析包含 19 种异氰酸酯测试物和 4,4'-二氨基二苯甲烷(MDA,4,4'-二苯基甲烷二异氰酸酯(MDI)过敏的标志物)的大型异氰酸酯斑贴试验系列的结果。
筛选异氰酸酯系列中的阳性反应测试文件。对阳性反应患者进行职业、暴露和诊断分析。
2010-2019 年,53 例患者在该系列中出现阳性反应(338 例测试患者的 16%)。MDA 是 MDI 过敏的成熟筛查物质,30 例患者呈阳性,23 例患者呈内部单体制剂 MDI 测试物质阳性,19-21 例患者呈 3 种不同的多体制剂 MDI 测试物质阳性。我们诊断了 16 例职业性变应性接触性皮炎(OACD),其中包括 3 名管道衬里工,来自 MDI 的六亚甲基-1,6-二异氰酸酯(HDI)齐聚物引起 5 例 OACD,比 2,4-甲苯二异氰酸酯(TDI;n=3)和异佛尔酮二异氰酸酯(IPDI;n=1)加起来还要多。
与以往研究不同,多体制剂 MDI 测试物质并不优于单体制剂 MDI。管道衬里工不仅可能因环氧树脂和丙烯酸酯产品致敏,还可能因 PU 管道涂层的固化剂中的 MDI 致敏。HDI 齐聚物是继 MDI 之后导致 OACD 的第二大重要原因。