Suppr超能文献

表面处理对树脂修复的树脂基CAD-CAM陶瓷粘结强度的影响:一项范围综述。

Effect of surface treatments on the bond strength of resin-repaired resin matrix CAD-CAM ceramic: A scoping review.

作者信息

Albergardi Ana Beatriz de Souza, Limírio João Pedro Justino de Oliveira, Gomes Jéssica Marcela de Luna, Pesqueira Aldiéris Alves, Pellizzer Eduardo Piza

机构信息

Department of Dental Materials and Prosthodontics, São Paulo State University (UNESP), Araçatuba, Brazil.

Department of Dental Materials and Prosthodontics, São Paulo State University (UNESP), Araçatuba, Brazil.

出版信息

J Dent. 2025 Mar;154:105594. doi: 10.1016/j.jdent.2025.105594. Epub 2025 Jan 30.

Abstract

OBJECTIVE

To evaluate the existing evidence on surface treatment techniques employed in the repair of resin matrix CAD-CAM ceramics and their effects on short- and long-term bond strength.

METHODOLOGY

This scoping review was conducted following the PRISMA-ScR guidelines for scoping reviews and was registered on the Open Science Framework platform. Based on the PCC concept, where P: Resin matrix CAD-CAM ceramic blocks for CAD-CAM, C: Bond strength, and C: Surface treatments, a search was conducted in the PubMed, Embase, Web of Science, Scopus, and Lilacs (grey literature) databases until October 2024, with no language or date restrictions.

RESULTS

In vitro studies comparing mechanical and/or chemical surface treatments on the bond strength of resin composite repairs were included. A total of 47 studies were included in the qualitative analysis, of which 45 used both mechanical and chemical treatments, and 29 used chemical treatments alone.

CONCLUSION

The combination of chemical and mechanical treatments is the appropriate option. Alumina blasting and silica coating are the most commonly used mechanical surface treatments, either alone or in conjunction with chemical treatments. Laser irradiation may serve as an alternative to conventional treatments.

CLINICAL SIGNIFICANCE

The studies revealed variability among protocols for repairing resin matrix CAD-CAM ceramics, with the combined use of chemical and mechanical treatments being the most effective approach.

摘要

目的

评估用于修复树脂基计算机辅助设计与制造(CAD-CAM)陶瓷的表面处理技术的现有证据及其对短期和长期粘结强度的影响。

方法

本综述性研究遵循PRISMA-ScR综述性研究指南进行,并在开放科学框架平台上注册。基于PCC概念,其中P:用于CAD-CAM的树脂基CAD-CAM陶瓷块,C:粘结强度,以及C:表面处理,在PubMed、Embase、科学网、Scopus和Lilacs(灰色文献)数据库中进行检索,截至2024年10月,无语言或日期限制。

结果

纳入了比较机械和/或化学表面处理对树脂复合材料修复粘结强度影响的体外研究。共有47项研究纳入定性分析,其中45项同时使用了机械和化学处理,29项仅使用了化学处理。

结论

化学和机械处理相结合是合适的选择。氧化铝喷砂和二氧化硅涂层是最常用的机械表面处理方法,可单独使用或与化学处理结合使用。激光照射可作为传统处理方法的替代方案。

临床意义

研究揭示了修复树脂基CAD-CAM陶瓷的方案存在差异,化学和机械处理联合使用是最有效的方法。