Tufekci E, Brantley W A, Mitchell J C, Foreman D W, Georgette F S
Ohio State University, Columbus, USA.
Int J Oral Maxillofac Implants. 1999 Sep-Oct;14(5):661-72.
The purpose of this study was to investigate the crystallographic characteristics of 3 sets of plasma-sprayed hydroxyapatite (HA) coatings prepared with different degrees of crystallinity on Ti-6Al-4V substrates. X-ray diffraction analyses were performed on the coatings to determine mean percent crystallinity, calcium phosphate phases present, average crystallite size, and residual strain. The mean percent crystallinity for the 3 sets of coatings ranged from 49 to 60%. The coatings that achieved the highest crystallinity consisted almost entirely of HA. As the coating crystallinity decreased, increasing amounts of alpha- and beta-tricalcium phosphate and tetracalcium phosphate were detected. The mean HA crystallite size for the 3 sets of coatings ranged from 0.02 to 0.05 micron. Differences in mean interplanar spacing for selected crystallographic planes of HA, compared with the pure ICDD (International Center for Diffraction Data) powder standards, implied that the coatings were in an uneven state of tensile strain.
本研究的目的是调查在Ti-6Al-4V基体上制备的3组具有不同结晶度的等离子喷涂羟基磷灰石(HA)涂层的晶体学特征。对涂层进行X射线衍射分析,以确定平均结晶度百分比、存在的磷酸钙相、平均晶粒尺寸和残余应变。3组涂层的平均结晶度百分比范围为49%至60%。结晶度最高的涂层几乎完全由HA组成。随着涂层结晶度降低,检测到越来越多的α-和β-磷酸三钙以及磷酸四钙。3组涂层的平均HA晶粒尺寸范围为0.02至0.05微米。与纯ICDD(国际衍射数据中心)粉末标准相比,HA选定晶面的平均面间距差异表明涂层处于不均匀的拉伸应变状态。