This study was conducted to determine the bond strength of some resin luting cements to zirconia ceramic. The hypothesis was that adhesive bonding capacity is influenced by different surface pretreatments designed for milled ceramic inlays.
Composite cylinders 5 mm x 5 mm were light cured on the ceramic surfaces for a shear test conducted in a test jig. Five surface treatments were studied: as received (from the milling machine), sandblasting with either 250- or 50-micron alumina sand, hydrofluoric acid treatment, and grinding with diamond burs. The tested luting cements were Panavia 21, Twinlook, and Superbond C&B.
All debonding occurred at the interface between ceramic and composite cement. Superbond demonstrated the highest bond strength regardless of the surface treatments. Grinding the surface with diamond burs improved the bonding slightly for Twinlook and Panavia 21 and also showed the roughest texture. Washing with hydrofluoric acid had no significant influence on bond strength.
Bond strengths for Twinlook and Pananvia 21 were quite low, and only Superbond showed a bond strength reasonably acceptable for clinical use; however, as no standard for bond strength has been established for inlay therapy, the other cements cannot be rejected as luting cements for inlays.
本研究旨在测定某些树脂粘结水门汀与氧化锆陶瓷的粘结强度。假设是,粘结能力受为研磨陶瓷嵌体设计的不同表面预处理的影响。
将5mm×5mm的复合圆柱体光固化在陶瓷表面,以便在测试夹具中进行剪切试验。研究了五种表面处理:原样接收(来自铣床)、用250微米或50微米氧化铝砂喷砂、氢氟酸处理以及用金刚石车针研磨。测试的粘结水门汀为Panavia 21、Twinlook和Superbond C&B。
所有脱粘均发生在陶瓷与复合水门汀的界面处。无论表面处理如何,Superbond均表现出最高的粘结强度。用金刚石车针研磨表面对Twinlook和Panavia 21的粘结略有改善,且表面纹理最粗糙。用氢氟酸冲洗对粘结强度无显著影响。
Twinlook和Pananvia 21的粘结强度相当低,只有Superbond表现出临床使用中合理可接受的粘结强度;然而,由于嵌体治疗尚未建立粘结强度标准,其他水门汀不能被排除作为嵌体的粘结水门汀。