Materials for interocclusal records and their ability to reproduce a 3-dimensional jaw relationship.

作者信息

Ockert-Eriksson G, Eriksson A, Lockowandt P, Eriksson O

机构信息

Department of Dental Biomaterial Science, Karolinska Institute, Huddinge, Sweden.

出版信息

Int J Prosthodont. 2000 Mar-Apr;13(2):152-8.

Abstract

PURPOSE

The purpose of this study was to determine if accuracy and dimensional stability of vinyl polysiloxanes and irreversible hydrocolloids stabilized by a tray used for fixed prosthodontics, removable partial, and complete denture cases are comparable to those of waxes and record rims and if storage time (24 hours or 6 days) affects dimensional stability of the tested materials.

MATERIALS AND METHODS

Two waxes, two record rims, three vinyl polysiloxanes, and one irreversible hydrocolloid (alginate) were examined. Three pairs of master casts with measuring steel rods were mounted on an articulator (initial position). Five records were made of each material, and the upper cast was remounted after 24 hours or 6 days so that deviations from the initial position could be measured.

RESULTS

Vinyl polysiloxanes reinforced by a stabilization tray were the most accurate materials able to reproduce a settled interocclusal position. Mounting casts (fixed prosthodontics cases) without records gave accuracy similar to wax records. Record rims used for removable partial and complete denture cases produced lesser accuracy than vinyl polysiloxanes and irreversible hydrocolloid stabilized by a tray. Accuracy was not significantly affected by storage time.

CONCLUSION

The results show that accuracy of vinyl polysiloxanes and irreversible hydrocolloids reinforced by a tray is superior to that of record rims with regard to the complete denture case and is among the most accurate with regard to the removable partial denture case. For fixed prosthodontics, however, reinforcement is unnecessary.

摘要

目的

本研究旨在确定用于固定修复、可摘局部义齿及全口义齿病例的托盘稳定的乙烯基聚硅氧烷和不可逆水胶体的准确性和尺寸稳定性是否与蜡及记录基托相当,以及储存时间(24小时或6天)是否会影响受试材料的尺寸稳定性。

材料与方法

对两种蜡、两种记录基托、三种乙烯基聚硅氧烷和一种不可逆水胶体(藻酸盐)进行检测。将三对带有测量钢棒的主模型安装在牙合架上(初始位置)。每种材料制作五份记录,24小时或6天后重新安装上半模型,以便测量与初始位置的偏差。

结果

用稳定托盘增强的乙烯基聚硅氧烷是能够重现稳定牙合间位置的最精确材料。未放置记录的安装模型(固定修复病例)的准确性与蜡记录相似。用于可摘局部义齿和全口义齿病例的记录基托的准确性低于用托盘稳定的乙烯基聚硅氧烷和不可逆水胶体。准确性不受储存时间的显著影响。

结论

结果表明,对于全口义齿病例,用托盘增强的乙烯基聚硅氧烷和不可逆水胶体的准确性优于记录基托;对于可摘局部义齿病例,其准确性是最高的之一。然而,对于固定修复,无需增强。