Takahashi Y, Chai J, Kawaguchi M
Department of Prosthodontics, Fukuoka Dental College, Fukuoka, Japan.
Int J Prosthodont. 2000 May-Jun;13(3):205-8.
This study was undertaken to characterize the long-term equilibrium flexural strength at proportional limit (FSp) of 4 denture reline polymers processed onto 4 denture base polymers.
A 3-point flexural test was applied on rectangular specimens of each denture base polymer-denture reline polymer. Each specimen was immersed in water for 4 months prior to and 4 months after reline.
Significant differences existed among the relined specimens because of the denture base polymer variable, the denture reline polymer variable, and their interaction (P < 0.05). The descending order in FSp according to the denture base polymer, arranged in terms of statistical significance was: Acron approximately Acron MC > Triad > Palapress Vario, where approximately denotes no significant difference between Acron and Acron MC. The descending order in FSp according to the denture reline polymer, arranged in terms of statistical significance was: Triad > Rebaron > Rebaron LC > Tokuso Rebase. Significant difference existed among all of the denture reline polymers.
The present study showed that the long-term equilibrium strengths of 4 denture reline polymers processed onto 4 denture base polymers were different. The strength of the relined specimen of a denture base is dependent on the strength of the denture base polymer and that of the reline polymer.
本研究旨在表征加工在4种义齿基托聚合物上的4种义齿重衬聚合物在比例极限下的长期平衡抗弯强度(FSp)。
对每种义齿基托聚合物-义齿重衬聚合物的矩形试件进行三点弯曲试验。每个试件在重衬前和重衬后均在水中浸泡4个月。
由于义齿基托聚合物变量、义齿重衬聚合物变量及其相互作用,重衬后的试件之间存在显著差异(P < 0.05)。根据义齿基托聚合物,按统计学显著性排列的FSp降序为:Acron约等于Acron MC > Triad > Palapress Vario,其中约等于表示Acron和Acron MC之间无显著差异。根据义齿重衬聚合物,按统计学显著性排列的FSp降序为:Triad > Rebaron > Rebaron LC > Tokuso Rebase。所有义齿重衬聚合物之间均存在显著差异。
本研究表明,加工在4种义齿基托聚合物上的4种义齿重衬聚合物的长期平衡强度不同。义齿基托重衬试件的强度取决于义齿基托聚合物和重衬聚合物的强度。