This study calculated the flexural strength for six reinforced restorative materials and demonstrated that flexural strength values can be determined simply by using physical parameters (diametral tensile strength and Young's modulus values) that are easily determined experimentally. A one-way ANOVA analysis demonstrated a statistically significant difference between the two reinforced glass ionomers and the four composite resin materials, with the composite resin being stronger than the glass ionomers.