Ineffective silane coupling between filler and matrix within dental composites is prone to accelerated in vivo degradation. In this study, we examined to what degree a procedure involving chemical decontamination of filler prior to silanization could improve the filler-matrix bonding, and thus the physico-mechanical properties, of composites. X-ray photoelectron spectroscopy revealed that filler-matrix coupling largely depended upon siloxane bridge (Si-O-Si) formation between the silica surface and the silane molecule, rather than on intermolecular bonding between adjacent silane molecules. Pre-silanization decontamination based upon boiling silica in 0.05-5% sodium peroxodisulfate, followed by ultrasonic rinsing in acetone, most effectively decontaminated filler. Consequently, it significantly improved the bonding of silane molecules to silanol groups at the silica surface. Experimental composites produced following pre-silanization decontamination of filler revealed a diametral tensile strength that was resistant to degradation by thermocycling.
牙科复合材料中填料与基体之间的硅烷偶联效果不佳容易导致体内加速降解。在本研究中,我们考察了在硅烷化之前对填料进行化学去污的程序能在多大程度上改善复合材料的填料-基体结合,进而改善其物理机械性能。X射线光电子能谱显示,填料-基体偶联很大程度上取决于二氧化硅表面与硅烷分子之间硅氧烷桥(Si-O-Si)的形成,而非相邻硅烷分子之间的分子间键合。基于在0.05-5%过二硫酸钠中煮沸二氧化硅,随后在丙酮中超声冲洗的硅烷化前去污方法,能最有效地对填料进行去污。因此,它显著改善了硅烷分子与二氧化硅表面硅醇基团的结合。填料经硅烷化前去污后制备的实验性复合材料显示出抗热循环降解的径向拉伸强度。