Erhardt Maria Carolina Guilherme, Magalhães Cláudia Silami, Serra Mônica Campos
Department of Restorative Dentistry, Piracicaba School of Dentistry, São Paulo, Brazil.
Oper Dent. 2002 Jul-Aug;27(4):396-402.
This in vitro study evaluated the effect of rebonding on microleakage of a resin composite, a condensable resin and two polyacid-modified resin composite restorations. Standardized cylindrical Class V dentin cavities were prepared on the buccal root surfaces of 240 extracted bovine incisive teeth. The prepared teeth were randomly assigned to four groups of 60 teeth and restored with the following restorative systems: I--(ZS) Z100/Scotchbond Multi-Purpose Plus; II--(SS) Solitaire/Solid Bond; III--(FS) Freedom/Stae; IV--(FSB) F200/Single Bond. Thirty teeth of each group were rebonded with a low-viscosity resin (Fortify/BISCO), according to the manufacturer's instructions. The remaining teeth received no treatment. All teeth were thermocycled for 5,000 cycles and brushed by hand three times a day for 10 days using a toothbrush and a slurry of dentifrice and water. Specimens were stained in a 2% methylene blue solution and longitudinally sectioned with diamond disks. Microleakage was scored on a scale of 0 to 3. The Kruskal-Wallis test showed statistically significant differences among the groups (h=156.54; alpha<0.05). Pairwise comparison by means of the least significant difference showed that (SS) and (FS) with or without rebonding were not statistically different from each other. These groups showed the highest microleakage differences from (ZS) and (FSB) with or without rebonding. (ZS) with rebonding showed the lowest microleakage that was not statistically different from (ZS) without rebonding and (FSB) with rebonding.
这项体外研究评估了再粘结对树脂复合材料、可压缩树脂和两种含多酸改性的树脂复合材料修复体微渗漏的影响。在240颗拔除的牛切牙的颊根表面制备标准化的圆柱形V类牙本质洞。将制备好的牙齿随机分为四组,每组60颗,并用以下修复系统进行修复:I组(ZS)Z100/多功能超强粘结剂;II组(SS)Solitaire/Solid Bond;III组(FS)Freedom/Stae;IV组(FSB)F200/单组分粘结剂。根据制造商的说明,每组中的30颗牙齿用低粘度树脂(Fortify/BISCO)进行再粘结。其余牙齿不进行处理。所有牙齿进行5000次热循环,每天用牙刷和牙膏与水的混合液手工刷牙3次,持续10天。将标本置于2%的亚甲蓝溶液中染色,并用金刚石切片机进行纵向切片。微渗漏程度按0至3级评分。Kruskal-Wallis检验显示各组之间存在统计学显著差异(h = 156.54;α<0.05)。通过最小显著差进行的两两比较表明,再粘结或未再粘结的(SS)组和(FS)组之间在统计学上无差异。这些组与再粘结或未再粘结的(ZS)组和(FSB)组相比,微渗漏差异最大。再粘结的(ZS)组显示出最低的微渗漏,与未再粘结的(ZS)组和再粘结的(FSB)组在统计学上无差异。