Johnson G H, Bales D J, Gordon G E, Powell L V
Department of Restorative Dentistry, University of Washington, School of Dentistry, Seattle, WA 98195.
Quintessence Int. 1992 Oct;23(10):705-11.
Two formulations of posterior composite resin (P-30 and Bisfil-P) were evaluated and compared to a high-copper, dispersed-phase amalgam (Dispersalloy). One hundred twenty-eight restorations were placed in 27 patients so that each patient received at least one of each material. After 3 years of clinical service, all three restorative materials produced clinically acceptable restorations, according to US Public Health Service and Leinfelder criteria. The amalgam restorations, however, underwent less wear (44 microns) than did the posterior composite resin restorations (60 to 74 microns). Stratification of data by type of tooth, class of restoration, and size of restoration produced the same ranking of wear from lowest to highest: Dispersalloy, Bisfil-P, and P-30. Resin restorations showed 45% more wear in molars than in premolars, and more wear was associated with moderately sized restorations than with conservative restorations. The surface texture of restorations of composite resin with porous strontium glass filler was nearly as smooth as that of enamel and was significantly smoother than that of the restorations of composite resin with zinc glass filler or of unpolished amalgam.
对两种后牙复合树脂配方(P - 30和Bisfil - P)进行了评估,并与一种高铜、分散相汞合金(Dispersalloy)进行比较。在27名患者中放置了128个修复体,以便每位患者至少接受每种材料中的一种。根据美国公共卫生服务部和莱因费尔德标准,经过3年的临床使用,所有三种修复材料都产生了临床上可接受的修复体。然而,汞合金修复体的磨损(44微米)比后牙复合树脂修复体(60至74微米)少。按牙齿类型、修复类别和修复体大小对数据进行分层,磨损程度从低到高的排名相同:Dispersalloy、Bisfil - P和P - 30。树脂修复体在磨牙中的磨损比在前磨牙中多45%,中等大小修复体的磨损比保守修复体更多。含多孔锶玻璃填料的复合树脂修复体的表面质地几乎与牙釉质一样光滑,并且明显比含锌玻璃填料的复合树脂修复体或未抛光汞合金修复体更光滑。