Abstract

Calcification is the most frequent cause of the clinical failure of bovine pericardium bioprosthetic valves, preventing their widespread application for surgical treatment. The aim of this study was to minimize calcific degeneration in bovine pericardium by using a chelating agent, ethylenediaminetetraacetic acid (EDTA). Freshly excised bovine pericardium was dissected free from adhering fat tissue and cut into 1-cm(2) pieces that were rinsed in phosphate-buffered saline solution (PBS) and transferred into 4 degrees C PBS containing 1% glutaraldehyde (GA) for initial fixation, then allocated into two groups. Group I received the same treatment in a fresh solution for 5 more days. Group II underwent an additional fixation step in PBS solution (pH 7.4, 37 degrees C) containing 11% EDTA for a period of 48 h (30 ml/g tissue) and was then transferred into freshly prepared PBS + 1% GA solution at 37 degrees C for another 3 days. To investigate the calcification rate, pericardial patches were inserted into the dorsal pouches of 25 male Wistar rats for 21 days. Calcium levels were measured with an atomic absorption spectrophotometer and examined histo-pathologically. The calcium content of EDTA-treated pericardium (Group II), 21 +/- 3.8 microg/mg, was significantly lower than that of Group I, 43.3 +/- 9.2 microg/mg. Assessment of the degree of calcification in the histological sections generally agreed well with the results of the chemical analyses. Calcium deposition in Group I samples were found to be solid mineral depositions, whereas in the Group II pericardial samples, only smaller traces of calcium were found. Calcific degeneration in bovine pericardium can be reduced by using chelates such as EDTA.

摘要

钙化是牛心包生物瓣膜临床失效的最常见原因,这阻碍了其在外科治疗中的广泛应用。本研究的目的是通过使用螯合剂乙二胺四乙酸(EDTA)来尽量减少牛心包的钙化变性。将刚切除的牛心包从附着的脂肪组织中分离出来,切成1平方厘米的小块,在磷酸盐缓冲盐溶液(PBS)中冲洗,然后转移到含有1%戊二醛(GA)的4℃ PBS中进行初步固定,随后分为两组。第一组在新鲜溶液中进行相同处理,持续5天。第二组在含有11% EDTA的PBS溶液(pH 7.4,37℃)中进行额外的固定步骤,持续48小时(30毫升/克组织),然后转移到37℃新制备的PBS + 1% GA溶液中,再处理3天。为了研究钙化率,将心包补片植入25只雄性Wistar大鼠的背部皮下袋中,持续21天。用原子吸收分光光度计测量钙水平,并进行组织病理学检查。经EDTA处理的心包(第二组)的钙含量为21±3.8微克/毫克,显著低于第一组的43.3±9.2微克/毫克。组织学切片中钙化程度的评估结果与化学分析结果基本一致。发现第一组样本中的钙沉积为固体矿物质沉积,而在第二组心包样本中,仅发现少量钙痕迹。通过使用EDTA等螯合剂可以减少牛心包的钙化变性。