Wang C X, Chen Z Q, Wang M
Department of Dental Materials, College of Stomatology, West China University of Medical Sciences, Chengdu 610041, Sichuan, China.
J Mater Sci Mater Med. 2002 Mar;13(3):247-51. doi: 10.1023/a:1014050715535.
Ion beam sputtering and ion beam sputtering/mixing deposition techniques were used to produce thin bioactive glass coatings on titanium substrate. It was found that as-deposited coatings were amorphous. Scanning electron microscopical examination showed that the coatings had a uniform and dense structure and that fabrication parameters affected the surface morphology of the coatings. The surface Ca/P ratio of the coatings, which varied from 5.9 to 8.6 according to semi-quantitative EDX analyses, was correlated with the fabrication condition. Depth profiling of the coatings revealed four distinct zones: the top surface, the thin coating zone, the intermixed zone of coating and substrate, and the substrate. Scratch tests showed that the coatings adhered well to the substrate.
采用离子束溅射和离子束溅射/混合沉积技术在钛基底上制备了生物活性玻璃薄膜涂层。结果发现,沉积态涂层为非晶态。扫描电子显微镜检查表明,涂层结构均匀致密,制备参数影响涂层的表面形貌。根据半定量能谱分析,涂层的表面钙/磷比在5.9至8.6之间变化,该比值与制备条件相关。涂层的深度剖析显示出四个不同的区域:顶面、薄涂层区、涂层与基底的混合区以及基底。划痕试验表明,涂层与基底结合良好。