Yassine Mahmoud M, Lucy Charles A
Department of Chemistry, University of Alberta, Gunning/Lemieux Chemistry Centre, Edmonton, Alberta, Canada T6G 2G2.
Anal Chem. 2005 Jan 15;77(2):620-5. doi: 10.1021/ac048909d.
Semipermanent coatings were generated within fused-silica capillaries by flushing the capillary with a 0.1 mM solution of the double-chained cationic surfactants didodecyldimethylammonium bromide, dimethylditetradecylammonium bromide (2C(14)DAB), dihexadecyldimethylammonium bromide, and dimethyldioctadecylammonium bromide (2C(18)DAB) and the triple-chained surfactant tridodecylmethylammonium iodide. All of these coatings were semipermanent, whereby the coating remained intact after the unadsorbed surfactant was removed from the capillary. The separation efficiencies for four model cationic proteins ranged from 1.2 to 1.4 million plates/m for the 2C(14)DAB coating to 0.3-0.4 million plates/m for the 2C(18)DAB coatings. The stability of the coating increased with increasing hydrophobicity of the surfactant (i.e., increasing chain length and decreasing cmc). Over 60 successive separations were performed on a 2C(18)DAB-coated capillary over 12 days, without any regeneration of the coating. The migration times varied by less than 2.3% over this period with no loss in efficiency.
通过用0.1 mM的双链阳离子表面活性剂双十二烷基二甲基溴化铵、二甲基二(十四烷基)溴化铵(2C(14)DAB)、二(十六烷基)二甲基溴化铵和二甲基二(十八烷基)溴化铵(2C(18)DAB)以及三链表面活性剂三(十二烷基)甲基碘化铵冲洗熔融石英毛细管,在其中生成了半永久性涂层。所有这些涂层都是半永久性的,即从毛细管中去除未吸附的表面活性剂后,涂层仍保持完整。对于四种模型阳离子蛋白,2C(14)DAB涂层的分离效率为120万至140万理论塔板数/米,而2C(18)DAB涂层的分离效率为30万至40万理论塔板数/米。涂层的稳定性随着表面活性剂疏水性的增加(即链长增加和临界胶束浓度降低)而提高。在12天内,对一根涂有2C(18)DAB的毛细管进行了60多次连续分离,涂层无需任何再生处理。在此期间,迁移时间的变化小于2.3%,且效率没有损失。