牙本质黏结剂和固化方式对间接修复体中牙本质膜厚度及与牙本质微拉伸黏结强度的影响。

The effect of dentin adhesive and cure mode on film thickness and microtensile bond strength to dentin in indirect restorations.

作者信息

Coelho Santos Maria Jacinta Moraes, Navarro Maria Fidela Lima, Tam Laura, McComb Dorothy

机构信息

Department of Dental Clinic, Faculty of Dentistry, Federal University of Bahia, Salvador, BA, Brazil.

出版信息

Oper Dent. 2005 Jan-Feb;30(1):50-7.

Abstract

This study evaluated the influence of dentin adhesive application technique (pre-curing vs non precuring) on microtensile bond strength (microTBS) to dentin and adhesive layer thickness in indirect resin restorations. Seven proprietary dentin adhesives were tested, including one-step and multistep products. Experimental groups included adhesive pre-cure (PC) with a halogen light source and no pre-cure (NPC) prior to resin cement insertion. Thirty caries-free molars received an MO inlay preparation. Inlays made with Tetric Ceram resin composite were cemented using a dual-cured resin luting agent. Prior to inlay cementation, each tooth was treated with one dentin bonding agent, using pre-cure (PC) or no pre-cure (NPC). After storage in distilled water at 37 degrees C for 24 hours, the teeth were sectioned along their long axis to produce serial sticks for microtensile bond strength testing at 0.5 mm/minute. The results were subjected to statistical analysis by one-way and two-way analysis of variance (ANOVA) and Tukey's multiple comparison test (p < or = 0.05). For the film thickness evaluation, 10 additional teeth were restored and sectioned mesiodistally. The thickness of the adhesive layer was evaluated by SEM at 1000x magnification at the pre-selected locations. The microTBS varied from 11.7 +/- 4.5 MPa to 43.4 +/- 9.8 MPa. The effect of pre-curing the adhesive was material specific. No adhesive layer was visualized for the adhesives used without the pre-curing step. The thickness of the adhesive layer for the pre-cured groups varied according to the different areas analyzed.

摘要

本研究评估了牙本质黏结剂应用技术(预固化与非预固化)对间接树脂修复体中牙本质微拉伸黏结强度(microTBS)及黏结剂层厚度的影响。测试了七种专利牙本质黏结剂,包括一步法和多步法产品。实验组包括在树脂水门汀插入前用卤素光源进行黏结剂预固化(PC)和不进行预固化(NPC)。30颗无龋磨牙进行了MO嵌体预备。用Tetric Ceram树脂复合材料制作的嵌体使用双固化树脂黏结剂黏结。在嵌体黏结前,每颗牙齿用一种牙本质黏结剂处理,采用预固化(PC)或不预固化(NPC)。在37℃蒸馏水中储存24小时后,沿牙齿长轴切片以制作系列小棒,用于以0.5mm/分钟的速度进行微拉伸黏结强度测试。结果通过单向和双向方差分析(ANOVA)以及Tukey多重比较检验进行统计分析(p≤0.05)。对于膜厚度评估,另外10颗牙齿进行修复并近远中向切片。在预选定位置通过扫描电子显微镜(SEM)以1000倍放大率评估黏结剂层的厚度。微拉伸黏结强度在11.7±4.5MPa至43.4±9.8MPa之间变化。黏结剂预固化的效果因材料而异。未进行预固化步骤所使用的黏结剂未观察到黏结剂层。预固化组黏结剂层的厚度根据所分析的不同区域而有所不同。