Suppr超能文献

空气喷砂预备对玻璃离子水门汀修复体微渗漏的影响。

Influence of air abrasion preparation on microleakage in glass ionomer cement restorations.

作者信息

Reis Lucia da Silva, Chinelatti Michelle A, Corona Silmara A M, Palma-Dibb Regina G, Borsatto Maria Cristina

机构信息

Ribeirão Preto School of Dentistry, University of São Paulo, Brazil.

出版信息

J Mater Sci Mater Med. 2004 Nov;15(11):1213-6.

Abstract

The aim of this study was to assess microleakage in class V cavities prepared by air abrasion or high-speed dental bur and restored with different glass ionomer cements. Sixty bovine incisors were equally divided into 6 groups: I, II and III (preparation by high-speed) and IV, V and VI (preparation by air abrasion). Groups I and IV were restored with Fuji IX; groups II and V with Ketac Molar; and groups III and VI with Vitremer. After 24 h (37 degrees C), specimens were thermocycled, isolated with nail varnish, immersed in a 0.2% Rhodamine B solution for 24 hours, sectioned longitudinally and analyzed for microleakage using an optical microscope connected to a digital camera and a computer. The images were digitized and a software allowed the quantitative evaluation of microleakage in millimeters. Data were analyzed by Wilcoxon and Kruskal-Wallis tests. It was observed that there were significant differences (p < 0.05) between incisal (enamel) and cervical (dentine/cementum) margins, mainly for Ketac Molar; there was no difference (p > 0.05) between preparation methods, except for group II (high-speed/Ketac Molar) that showed higher infiltration; regarding the materials, Ketac Molar demonstrated the highest microleakage values (p < 0.05), and only Vitremer sealed completely both margins of restorations. It was concluded that air abrasion preparation did not influence microleakage in class V restorations with the employed glass ionomer cements.

摘要

本研究的目的是评估用空气磨蚀或高速牙钻制备的V类洞,并用不同玻璃离子水门汀修复后的微渗漏情况。60颗牛切牙平均分为6组:I、II和III组(高速制备)以及IV、V和VI组(空气磨蚀制备)。I组和IV组用Fuji IX修复;II组和V组用Ketac Molar修复;III组和VI组用Vitremer修复。24小时后(37摄氏度),对标本进行热循环处理,用指甲油隔离,浸入0.2%的罗丹明B溶液中24小时,纵向切片,并用连接数码相机和计算机的光学显微镜分析微渗漏情况。图像被数字化,一种软件可对微渗漏进行以毫米为单位的定量评估。数据通过Wilcoxon检验和Kruskal-Wallis检验进行分析。结果发现,切缘(釉质)和颈部(牙本质/牙骨质)边缘之间存在显著差异(p < 0.05),主要是Ketac Molar;除II组(高速/Ketac Molar)显示出较高的渗透外,制备方法之间没有差异(p > 0.05);关于材料,Ketac Molar显示出最高的微渗漏值(p < 0.05),只有Vitremer完全封闭了修复体的两个边缘。得出的结论是,在所使用的玻璃离子水门汀中,空气磨蚀制备对V类修复体的微渗漏没有影响。