Suppr超能文献

粘结系统与釉质和牙本质的剪切粘结强度。热循环的影响。

Shear bond strength of adhesive systems to enamel and dentin. Thermocycling influence.

作者信息

Dos Santos Patrícia Aleixo, Garcia Patrícia Petromilli Nordi Sasso, Palma-Dibb Regina Guenka

机构信息

Department of Operative Dentistry, Bauru School of Dentistry, University of São Paulo, Brazil.

出版信息

J Mater Sci Mater Med. 2005 Aug;16(8):727-32. doi: 10.1007/s10856-005-2609-2.

Abstract

OBJECTIVES

The purpose of the this study was to evaluate the influence of thermocycling on shear bond strength on bovine enamel and dentin surfaces of different adhesive systems.

METHODS

Thirty sound bovine incisors were sectioned in mesiodistal and inciso-cervical direction obtaining 60 incisal surfaces (enamel) and 60 cervical surfaces (dentin). Specimens were randomly assigned to 3 groups of equal size (n=40), according to the adhesive system used: I-Single Bond; II-Prime & Bond NT/NRC; III-One Coat Bond. After 24-h storage in distilled water at 37 degrees C, each main group was divided into two subgroups: A-specimens tested after 24 h storage in distilled water at 37 degrees C; B-specimens submitted to thermocycling (500 cycles). Shear bond strength tests were performed. Data were submitted to ANOVA and Tukey test.

RESULTS

Means (MPa) of different groups were: I-AE-16.96, AD-17.46; BE-21.60, BD-12.79; II-AE-17.20, AD-11.93; BE-20.67, BD-13.94; III-AE-25.66, AD-17.53; BE-24.20, BD-19.38.

SIGNIFICANCE

Thermocycling did not influence significantly the shear bond strength of the tested adhesive systems; enamel was the dental substrate that showed larger adhesive strength; One Coat Bond system showed the best adhesive strength averages regardless of substrate or thermocycling.

摘要

目的

本研究旨在评估热循环对不同粘结系统在牛牙釉质和牙本质表面剪切粘结强度的影响。

方法

将30颗完好的牛切牙沿近远中方向和切颈方向切开,获得60个切端表面(釉质)和60个颈部表面(牙本质)。根据所使用的粘结系统,将标本随机分为3组,每组大小相等(n = 40):I-单键粘结;II-预处理粘结剂NT/NRC;III-一层粘结剂。在37℃蒸馏水中储存24小时后,每个主要组再分为两个亚组:A-在37℃蒸馏水中储存24小时后测试的标本;B-进行热循环(500次循环)的标本。进行剪切粘结强度测试。数据进行方差分析和Tukey检验。

结果

不同组的平均值(MPa)为:I-A组釉质-16.96,牙本质-17.46;B组釉质-21.60,牙本质-12.79;II-A组釉质-17.20,牙本质-11.93;B组釉质-20.67,牙本质-13.94;III-A组釉质-25.66,牙本质-17.53;B组釉质-24.20,牙本质-19.38。

意义

热循环对测试粘结系统的剪切粘结强度没有显著影响;釉质是显示出较大粘结强度的牙体组织;无论牙体组织或热循环如何,一层粘结剂系统显示出最佳的粘结强度平均值。