Wataha J C, Craig R G, Hanks C T
University of Michigan School of Dentistry, Ann Arbor 48109-1078.
J Dent Res. 1992 Jul;71(7):1417-22. doi: 10.1177/00220345920710071101.
The kinetics of the release of elements from six dental casting alloys into cell-culture medium was assessed by means of atomic absorption spectroscopy. Alloys were evaluated in the polished and polished-cleaned conditions so that the effects of cleaning could be determined. Auger scanning microscopy was used for analysis of the surfaces of selected alloys before and after exposure to the cell-culture medium. Release patterns for each element were characterized by the shape of the dissolution vs. time curve, concentration of the element at 12 h as a percentage of the 72-hour concentration, and the relative slope of the curve from 48 to 72 h. Three patterns of release were observed for elements in these alloys. Type I patterns had logarithmic shapes with relatively large 12-hour concentrations and low 48-72-hour slopes. Type II patterns had logarithmic shapes but with moderate 12-hour concentrations and 48-72-hour slopes. Type III patterns were polynomial in shape, had relatively low 12-hour concentrations, and had large 48-72-hour slopes. Cleaning did not change the pattern of release but did generally significantly decrease the quantities of elements released (p = 0.05). The type of dissolution vs. time curve appeared to be dependent upon the element and the composition of the alloy. When cleaning reduced dissolution, surface analyses showed that the cleaning process increased the abundance of elements such as Au and Pd and reduced the abundance of Ag and Cu. Elements which were released from the alloys were more abundant on the surface than in the bulk in both polished and polished-cleaned conditions.(ABSTRACT TRUNCATED AT 250 WORDS)
通过原子吸收光谱法评估了六种牙科铸造合金中元素释放到细胞培养基中的动力学。对合金在抛光和抛光清洁条件下进行评估,以便确定清洁的效果。使用俄歇扫描显微镜分析选定合金在暴露于细胞培养基前后的表面。每种元素的释放模式通过溶解与时间曲线的形状、12小时时元素浓度占72小时浓度的百分比以及48至72小时曲线的相对斜率来表征。在这些合金中的元素观察到三种释放模式。I型模式呈对数形状,12小时浓度相对较高,48至72小时斜率较低。II型模式呈对数形状,但12小时浓度和48至72小时斜率适中。III型模式呈多项式形状,12小时浓度相对较低,48至72小时斜率较大。清洁并没有改变释放模式,但通常确实显著减少了释放的元素量(p = 0.05)。溶解与时间曲线的类型似乎取决于元素和合金的组成。当清洁减少溶解时,表面分析表明清洁过程增加了金和钯等元素的丰度,降低了银和铜的丰度。在抛光和抛光清洁条件下,从合金中释放的元素在表面上比在整体中更丰富。(摘要截断于250字)