Suppr超能文献

贵金属烤瓷冠的金属-瓷修复失败:私人诊所一项前瞻性临床试验的7年结果

Metal-ceramic failure in noble metal crowns: 7-year results of a prospective clinical trial in private practices.

作者信息

Reitemeier Bernd, Hänsel Kristina, Kastner Christian, Walter Michael H

机构信息

Department of Prosthetic Dentistry, School of Dentistry, Dresden University of Technology, Dresden, Germany.

出版信息

Int J Prosthodont. 2006 Jul-Aug;19(4):397-9.

Abstract

PURPOSE

The aim of this study was to evaluate the clinical performance of metal-ceramic crowns placed in 10 private practices.

MATERIALS AND METHODS

In this prospective clinical trial, 95 patients were provided with 190 noble-metal metal-ceramic single crowns.

RESULTS

The 7-year survival rates of the crowns were 95.5% (target event: any removal), 99.5% (target event: removal because of defective veneer), and 92.4% (target event: metal-ceramic complication of any kind). No significant explanatory variables for metal-ceramic complications could be detected by bivariate and multivariate testing. The consequences resulting from metal-ceramic defects were of minor clinical significance in most cases.

CONCLUSION

The findings support previous claims that metal-ceramic restorations perform very well clinically, including in practices outside academic environments.

摘要

目的

本研究的目的是评估在10家私人诊所中放置的金属烤瓷冠的临床性能。

材料与方法

在这项前瞻性临床试验中,为95名患者提供了190颗贵金属金属烤瓷单冠。

结果

这些冠的7年生存率分别为95.5%(目标事件:任何移除情况)、99.5%(目标事件:因饰面缺陷而移除)和92.4%(目标事件:任何类型的金属烤瓷并发症)。通过双变量和多变量测试未检测到金属烤瓷并发症的显著解释变量。在大多数情况下,金属烤瓷缺陷导致的后果在临床上意义不大。

结论

这些发现支持了先前的说法,即金属烤瓷修复体在临床上表现良好,包括在学术环境之外的诊所。