The biomimetic coating method was used for fabricating calcium phosphate fibres for biomedical applications such as bone defect fillers. Natural cotton substrate was pre-treated with phosphorylation and a Ca(OH)2 saturated solution. The pre-treated samples were then soaked in simulated body fluid (SBF) of two different concentrations, 1.5 times and 5.0 times the ion concentration of blood plasma. The cotton was then burnt out via sintering of the ceramic coating at 950 degrees C, 1050 degrees C, 1150 degrees C, and 1250 degrees C. The results demonstrated that osteoblastic cells were able to cover the entire surface cotton fibres, and the cell coverage appeared to be independent of surface roughness and Ca/P ratio of fibres.
采用仿生涂层法制备用于生物医学应用(如骨缺损填充剂)的磷酸钙纤维。天然棉基材先用磷酸化和氢氧化钙饱和溶液进行预处理。然后将预处理后的样品浸泡在两种不同浓度(分别为血浆离子浓度的1.5倍和5.0倍)的模拟体液(SBF)中。接着通过在950℃、1050℃、1150℃和1250℃下烧结陶瓷涂层将棉花烧掉。结果表明,成骨细胞能够覆盖整个棉纤维表面,并且细胞覆盖率似乎与纤维的表面粗糙度和钙磷比无关。