Chen Qian-huo, Zhang Wen-gong
College of Chemistry and Materials Science, Fujian Normal University, Fuzhou, 350007, PR China.
J Colloid Interface Sci. 2007 May 15;309(2):531-7. doi: 10.1016/j.jcis.2006.10.069. Epub 2006 Nov 1.
Alumina 8-hydroxyquinoline complexes (Alqx)/Al2O3 nano colloids have been successfully prepared by focused, pulsed laser ablation at the interface of solid Al2O3 and a flowing liquid containing 8-hydroxyquinoline (Q) and one of two polymers (polystyrene, PS, and polymethyl methacrylate, PMMA). Three factors influenced the luminescence of the (Alqx)/Al2O3 nano colloids. The first factor was whether the 8-hydroxyquinoline was added before or after laser ablation. The second factor was if the reaction medium consisted of (1) Q dissolved in ethanol, (2) Q dissolved in cyclohexane containing PS, or (3) Q dissolved in ethyl acetate containing PMMA. The third factor affecting luminescence was the age of the colloids. The (Alqx)/Al2O3 nano colloid product was characterized by transmission electron microscopy (TEM), ultraviolet visible spectroscopy (UV-vis), X-ray diffraction (XRD), X-ray photoelectron spectroscopy (XPS) and fluorescence spectroscopy. The product from all three-reaction media luminesced when irradiated with ultraviolet light. The product formed in cyclohexane containing PS gave the greatest luminescence, followed by the product formed in ethanol, and the product formed in ethyl acetate containing PMMA gave the smallest luminescence. The luminescence mechanism is similar to that of Alq3.
通过在固体Al2O3与含有8-羟基喹啉(Q)以及两种聚合物(聚苯乙烯,PS,和聚甲基丙烯酸甲酯,PMMA)之一的流动液体的界面处进行聚焦脉冲激光烧蚀,成功制备了氧化铝8-羟基喹啉配合物(Alqx)/Al2O3纳米胶体。三个因素影响了(Alqx)/Al2O3纳米胶体的发光。第一个因素是8-羟基喹啉是在激光烧蚀之前还是之后添加。第二个因素是反应介质是否由(1)溶解在乙醇中的Q、(2)溶解在含有PS的环己烷中的Q或(3)溶解在含有PMMA的乙酸乙酯中的Q组成。影响发光的第三个因素是胶体的老化程度。(Alqx)/Al2O3纳米胶体产物通过透射电子显微镜(TEM)、紫外可见光谱(UV-vis)、X射线衍射(XRD)、X射线光电子能谱(XPS)和荧光光谱进行表征。当用紫外光照射时,来自所有三种反应介质的产物都会发光。在含有PS的环己烷中形成的产物发出的光最强,其次是在乙醇中形成的产物,而在含有PMMA的乙酸乙酯中形成的产物发出的光最弱。发光机制与Alq3的相似。