Suppr超能文献

泡桐(Paulownia fortunei L.)自水解和制浆工艺增值的新视角。

New perspectives for Paulownia fortunei L. valorisation of the autohydrolysis and pulping processes.

作者信息

Caparrós S, Díaz M J, Ariza J, López F, Jiménez L

机构信息

Departamento de Ingeniería Química, Campus del Carmen, Universidad de Huelva, Huelva, Spain.

出版信息

Bioresour Technol. 2008 Mar;99(4):741-9. doi: 10.1016/j.biortech.2007.01.028. Epub 2007 Mar 26.

Abstract

This paper will consider the influence of the temperature of autohydrolysis or hydrothermal process from Paulownia fortunei L. to obtain a valuable liquid phase and a suitable solid phase to produce pulp. The solid phase resulting of autohydrolysis was subjected to organosolv pulping process and formed paper sheets, analyzing the influence of operational variables (viz., ethanol concentration, temperature and pulping time) on the yield, viscosity, tensile index, burst index, tear index and brightness. Maximum glucose and xylose contents and minimum paper sheets characteristic loss have been obtained at 190 degrees C authohydrolysis temperature. Suitable characteristics of paper sheets and acceptable yield, viscosity and kappa number of pulp could be obtained by operating at 180 degrees C temperature, 30min pulping time and 20% ethanol concentration. Under those conditions sheets paper with 27.4% ISO brightness, 28.87Nm/g tensile index, 1.22kPam(2)/g burst index and 1.23kNm(2)/g tear index could be obtained.

摘要

本文将探讨来自泡桐的自水解或水热过程的温度对获取有价值的液相和合适的固相以生产纸浆的影响。自水解产生的固相进行有机溶剂制浆过程并制成纸张,分析操作变量(即乙醇浓度、温度和制浆时间)对得率、粘度、拉伸指数、耐破指数、撕裂指数和亮度的影响。在190℃自水解温度下获得了最大的葡萄糖和木糖含量以及最小的纸张特性损失。通过在180℃温度、30分钟制浆时间和20%乙醇浓度下操作,可以获得合适的纸张特性以及可接受的纸浆得率、粘度和卡伯值。在这些条件下,可以获得具有27.4%ISO亮度、28.87Nm/g拉伸指数、1.22kPam²/g耐破指数和1.23kNm²/g撕裂指数的纸张。