Abstract

Hydrothermal processing of Eucalyptus wood was performed at operation temperature of 181 degrees C, processing time or 37.5 min and solid water ratio of 1/6 to ensure a maximum loss of xylan recuperation with minimum cellulose fibre degradation. Under those conditions, the loss of xylan was 22% less than that achieved with the conditions 196 degrees C, 50.6 min and 1/8 (solid/water). IN In addition, an experimental design was used to study the influence of process variables: temperature (145-175 degrees C), pulping time (40-120 min) and ethanol concentration (40-70% weight concentration), on the properties of pulps (yield, kappa number, viscosity, cellulose, xylan, lignin acetyl groups contents and brightness) and paper sheets (stretch index, burst index and tear index) obtained from the solid fraction after hydrothermal treatment of Eucalyptus globulus. Pulps with acceptably high physical and chemical properties can be obtained operating at 175 degrees C for 90 min with 55% ethanol concentration.

摘要

对桉木进行水热加工时,操作温度为181摄氏度,处理时间为37.5分钟,固水比为1/6,以确保木聚糖回收率损失最大且纤维素纤维降解最小。在这些条件下,木聚糖的损失比在196摄氏度、50.6分钟和1/8(固/水)条件下减少了22%。此外,采用实验设计研究了工艺变量(温度145 - 175摄氏度、制浆时间40 - 120分钟和乙醇浓度40 - 70%重量浓度)对从蓝桉水热处理后的固体部分获得的纸浆(得率、卡伯值、粘度、纤维素、木聚糖、木质素乙酰基含量和亮度)和纸张(拉伸指数、耐破指数和撕裂指数)性能的影响。在175摄氏度下操作90分钟,乙醇浓度为55%时,可获得具有可接受的高物理和化学性能的纸浆。

文献AI研究员

20分钟写一篇综述,助力文献阅读效率提升50倍。

立即体验

用中文搜PubMed

大模型驱动的PubMed中文搜索引擎

马上搜索

文档翻译

学术文献翻译模型,支持多种主流文档格式。

立即体验