To assess the shear bond strength of resin composite to human enamel and dentin after using a whitening dentifrice containing carbamide peroxide for 21 days.
Thirty enamel and 30 dentin slabs were embedded, flattened and randomly divided into three groups (n=10) that received different treatments: carbamide peroxide containing dentifrice (Rembrandt Plus), fluoride containing dentifrice (Close Up with fluoride), and immersion in artificial saliva as the control group. Applications were made for a 15-minute period daily, immersing the slabs in a suspension with distilled water and dentifrice in the ratio of 3:1 (weight) for 21 days. For the rest of the time, the slabs were kept in an artificial saliva solution. After the last application, an adhesive system (Single Bond) was used to bond resin-based composite cylinders (Z100) to the enamel and dentin surfaces for the shear bond strength tests. These tests were carried out in a universal testing machine at a speed of 0.5 mm/minute.
ANOVA and the Tukey test for enamel and Kruskal-Wallis and the Dunn Method for dentin, showed significant differences between slabs treated with Rembrandt Plus (REM) and the artificial saliva control group, with higher values for REM (P < 0.05). There were no differences in mean bond strengths of enamel and dentin treated with Close Up with fluoride (CLO) and REM, nor were any differences shown between CLO and the artificial saliva control group. A whitening dentifrice containing carbamide peroxide increased the bond strength of restorative systems.
评估使用含过氧化脲的美白牙膏21天后树脂复合材料与人类牙釉质和牙本质的剪切粘结强度。
将30块牙釉质和30块牙本质片进行包埋、打磨平整,随机分为三组(n = 10),分别接受不同处理:含过氧化脲的牙膏(Rembrandt Plus)、含氟牙膏(含氟的Close Up),以及浸入人工唾液作为对照组。每天进行15分钟的处理,将牙片浸入蒸馏水与牙膏重量比为3:1的悬浮液中21天。其余时间,将牙片保存在人工唾液溶液中。在最后一次处理后,使用粘结系统(Single Bond)将树脂基复合材料圆柱体(Z100)粘结到牙釉质和牙本质表面,进行剪切粘结强度测试。这些测试在万能试验机上以0.5毫米/分钟的速度进行。
牙釉质的方差分析和Tukey检验以及牙本质的Kruskal-Wallis检验和Dunn方法显示,使用Rembrandt Plus(REM)处理的牙片与人工唾液对照组之间存在显著差异,REM组的值更高(P < 0.05)。用含氟的Close Up(CLO)和REM处理的牙釉质和牙本质的平均粘结强度没有差异,CLO组与人工唾液对照组之间也没有差异。含过氧化脲的美白牙膏提高了修复系统的粘结强度。