Suppr超能文献

用于偶氮染料降解的嵌入高度有序TiO(2)纳米管阵列电极中的ZnO纳米棒的制备及其光电催化活性

Preparation and photoelectrocatalytic activity of ZnO nanorods embedded in highly ordered TiO(2) nanotube arrays electrode for azo dye degradation.

作者信息

Zhang Zhonghai, Yuan Yuan, Liang Linhong, Cheng Yuxiao, Shi Guoyue, Jin Litong

机构信息

Department of Chemistry, East China Normal University, Shanghai 200062, China.

出版信息

J Hazard Mater. 2008 Oct 30;158(2-3):517-22. doi: 10.1016/j.jhazmat.2008.01.118. Epub 2008 Mar 10.

Abstract

In this article, the ZnO nanorods embedded in highly ordered TiO(2) nanotube arrays (ZnO/TiO(2) NR/Ts) electrodes were fabricated through two steps: (1) electrosynthesis of TiO(2) nanotube arrays (TiO(2) NTs) in HF solution by anodization method; (2) followed by cathodic electrodeposition of ZnO embedded in the TiO(2) nanotube arrays. The morphological characteristics and structures of ZnO/TiO(2) NR/Ts electrodes were examined by field-emission scanning electron microscopy (FE-SEM), energy dispersive X-ray (EDX) spectroscopy, X-ray diffraction (XRD) analysis, and UV-vis spectra. The linear-sweep photovoltammetry response on the ZnO/TiO(2) NR/Ts electrode was presented and the photocurrent was dramatically enhanced on the ZnO/TiO(2) NR/Ts electrode, comparing with that on bare TiO(2) NTs electrode. The photocatalytic and photoelectrocatalytic activity of ZnO/TiO(2) NR/Ts electrode was evaluated in degradation of methyl orange (MO) in aqueous solution.

摘要

在本文中,通过两步法制备了嵌入高度有序二氧化钛纳米管阵列(ZnO/TiO₂ NR/Ts)电极中的氧化锌纳米棒:(1)采用阳极氧化法在氢氟酸溶液中电合成二氧化钛纳米管阵列(TiO₂ NTs);(2)随后在二氧化钛纳米管阵列中进行阴极电沉积嵌入氧化锌。通过场发射扫描电子显微镜(FE-SEM)、能量色散X射线(EDX)光谱、X射线衍射(XRD)分析和紫外可见光谱对ZnO/TiO₂ NR/Ts电极的形态特征和结构进行了研究。给出了ZnO/TiO₂ NR/Ts电极上的线性扫描光电流响应,与裸TiO₂ NTs电极相比,ZnO/TiO₂ NR/Ts电极上的光电流显著增强。在水溶液中甲基橙(MO)的降解实验中评估了ZnO/TiO₂ NR/Ts电极的光催化和光电催化活性。