Suppr超能文献

动脉内注射牙髓用氢氧化钙后的严重组织坏死:病例系列

Severe tissue necrosis following intra-arterial injection of endodontic calcium hydroxide: a case series.

作者信息

Sharma Sanjay, Hackett Robert, Webb Roger, Macpherson David, Wilson Alan

机构信息

St Richards Hospital, Chichester, West Sussex, UK.

出版信息

Oral Surg Oral Med Oral Pathol Oral Radiol Endod. 2008 May;105(5):666-9. doi: 10.1016/j.tripleo.2007.11.026.

Abstract

We present 2 cases of intra-arterial injection of endodontic calcium hydroxide via the root canal system of molar teeth. Nonsetting calcium hydroxide paste was used as a temporary dressing during endodontic treatment and in both cases delivered via an injectable syringe technique. Retrograde flow of the calcium hydroxide occurred along the artery until its origin where orthograde flow continued to the capillary bed. Case 1 demonstrates calcium hydroxide injected into the distal root canal of a lower second molar resulting in its distribution to the external carotid bed and case 2 demonstrates calcium hydroxide injected into the palatal root of an upper second molar with flow into the infraorbital artery. In both cases this resulted in severe clinical signs and symptoms ending in tissue necrosis. Long-term sequelae included scarring, deformity, and chronic pain. This case series illustrates the high toxicity of calcium hydroxide when displaced into vessels and soft tissues. Caution should be exercised when using injectable systems for endodontic calcium hydroxide.

摘要

我们报告了2例通过磨牙根管系统进行动脉内注射牙髓用氢氧化钙的病例。非凝固性氢氧化钙糊剂在牙髓治疗期间用作临时敷料,在这2例病例中均通过可注射注射器技术给药。氢氧化钙沿动脉逆行流动,直至其起源处,然后顺行流向毛细血管床。病例1显示氢氧化钙注入下颌第二磨牙的远中根管,导致其分布至颈外动脉床;病例2显示氢氧化钙注入上颌第二磨牙的腭根,并流入眶下动脉。在这2例病例中,这均导致了严重的临床体征和症状,最终导致组织坏死。长期后遗症包括瘢痕形成、畸形和慢性疼痛。该病例系列说明了氢氧化钙进入血管和软组织时的高毒性。在使用可注射系统进行牙髓用氢氧化钙治疗时应谨慎。