Chang Shwu Jen, Kuo Shyh Ming, Manousakas Ioannis, Niu Gregory Cheng-Chie, Chen Jin Pin
Department of Biomedical Engineering, I-SHOU University, Kaohsiung County 840, Taiwan.
Acta Biomater. 2009 Jan;5(1):101-14. doi: 10.1016/j.actbio.2008.08.002. Epub 2008 Aug 20.
Collagen II and hyaluronan are the two major components of the native extracellular matrix (ECM). Both biopolymers are responsible for providing the associated tissues with tensile strength, and also serve as a structural scaffold for cell adhesion and growth. Over the years, many researchers have focused on the preparation and evaluation of man-made ECM comprising the two polymers in the form of a membrane for chondrocyte culture applications. Here, a simple and in situ method, involving the injection of the hyaluronan/collagen II (HA/Col II) mixture solution through a pair of hollow-centered parallel disc electrodes (HCPDEs) of a high-voltage electrostatic field system, was developed and employed to prepare HA/Col II microspheres in watery phase. The HA/Col II microspheres were firmed up by a two-step cross-linking treatment (first by FeCl(3) and then by 1-ethyl-3-(3-dimethyl aminopropyl) carbodimide, EDC) to secure the spherical structure shape. Then, at 37 degrees C, reconstitution treatment of the Col II molecules was conducted to further strengthen the microspheres. Depending on treatment conditions, the resulting series of HA/Col II microspheres all exhibited good sphericity in the range of 486+/-43 to 679+/-24microm in diameter. Furthermore, the ratio and amount of HA/Col II in the mixture solutions would affect the morphological structure and basic characteristics, including mechanical strength, thermal properties and water content. In the preliminary study, the HA/Col II microspheres have shown to provide favorable ECM characteristics, with appropriate mechanical strength, and exhibited a 3D inclination.
胶原蛋白II和透明质酸是天然细胞外基质(ECM)的两种主要成分。这两种生物聚合物都负责为相关组织提供抗张强度,并且还作为细胞粘附和生长的结构支架。多年来,许多研究人员专注于制备和评估由这两种聚合物以膜的形式组成的人造ECM,用于软骨细胞培养应用。在此,开发并采用了一种简单的原位方法,即通过高压静电场系统的一对空心平行圆盘电极(HCPDEs)注入透明质酸/胶原蛋白II(HA/Col II)混合溶液,以在水相中制备HA/Col II微球。通过两步交联处理(首先用FeCl(3),然后用1-乙基-3-(3-二甲基氨基丙基)碳二亚胺,EDC)使HA/Col II微球固化,以确保球形结构形状。然后,在37℃下,对Col II分子进行重构处理以进一步强化微球。根据处理条件,所得的一系列HA/Col II微球在直径486±43至679±24μm范围内均表现出良好的球形度。此外,混合溶液中HA/Col II的比例和量会影响形态结构和基本特性,包括机械强度、热性能和含水量。在初步研究中,HA/Col II微球已显示出具有良好的ECM特性,具有适当的机械强度,并呈现出三维倾斜度。