Suppr超能文献

储水时间对酸蚀冲洗型和自酸蚀型粘结系统粘结强度的影响。

Influence of water storage time on the bond strength of etch-and-rinse and self-etching adhesive systems.

作者信息

Dantas Darlene Cristina Ramos Eloy, Ribeiro Ana Isabella Arruda Meira, Lima Lúcia Helena Marques de Almeida, de Lima Marcelino Guedes, Guênes Gymenna Maria Tenório, Braz Ana Karla Souza, Braz Rodivan

机构信息

Department of Dentistry, State University of Paraíba, Campina Grande, PB, Brazil.

出版信息

Braz Dent J. 2008;19(3):219-23. doi: 10.1590/s0103-64402008000300008.

Abstract

The purpose of this study was to evaluate comparatively the shear bond strength (SBS) of etch-and-rinse (Adper Scotch Bond Multi Purpose--ASBMP and Adper Single Bond 2--ASB2) and self-etching (AdheSe--AD and Adper Prompt--AP) adhesive systems after short- and long-term water storage. Eighty bovine teeth were randomly assigned to 4 groups (n=20, 10 teeth for 24 h and 10 for 6 months). After surface treatment, composite resin cylinders were made with Tetric Ceram using a bisected metallic matrix. The specimens were stored in distilled water at 37 degrees C for either 24 h or 6 months. After these periods, shear strength was assessed in a universal testing machine (0.5 mm/min). Data were submitted to ANOVA and F test at 5% significance level. Mean SBSs (MPa) for ASBMP (10.03 +/- 3.78) and ASB2 (6.10 +/- 2.67) showed no statistically significant differences (p>0.05) between times. The self-etching systems did not differ significantly from each other within the 24-h period, but significant difference was found for AD (1.37 +/- 0.64) after 6 months of water storage. In conclusion, the tested etch-and-rinse systems had a better performance in terms of bond durability over time than the self-etching systems.

摘要

本研究的目的是比较短期和长期水储存后,酸蚀冲洗型(Adper Scotch Bond Multi Purpose——ASBMP和Adper Single Bond 2——ASB2)和自酸蚀型(AdheSe——AD和Adper Prompt——AP)粘结系统的剪切粘结强度(SBS)。80颗牛牙被随机分为4组(n = 20,其中10颗牙储存24小时,10颗牙储存6个月)。表面处理后,使用对半金属模具,用Tetric Ceram制作复合树脂圆柱体。将样本在37℃的蒸馏水中储存24小时或6个月。在这些时间段后,在万能试验机上(以0.5毫米/分钟的速度)评估剪切强度。数据在5%显著性水平下进行方差分析和F检验。ASBMP(10.03±3.78)和ASB2(6.10±2.67)的平均SBS在不同时间之间无统计学显著差异(p>0.05)。自酸蚀系统在24小时内彼此之间无显著差异,但在水储存6个月后,AD(1.37±0.64)有显著差异。总之,就粘结耐久性而言,经测试的酸蚀冲洗型系统随时间推移比自酸蚀型系统表现更好。