Osman Saad A, McCabe John F, Walls Angus W G
School of Dental Sciences, Newcastle University, Newcastle upon Tyne, UK.
Eur J Prosthodont Restor Dent. 2008 Dec;16(4):166-70.
The shear bond strength of three adhesives, Panavia 21, Superbond, All Bond C&B Cement, and Variolink (a dual cure resin) to various dentine depths were determined. Fifteen human fully erupted permanent first and second molars were wet ground using 500 and then 800 grit abrasive papers to expose the superficial, middle and the deep dentine, for each adhesive tested. Five samples were prepared for each dentine depth. The adhesives were bonded to the samples using gelatine capsules and were matured for 24 h in water at 37 degrees C. The samples were debonded in shear using tensile testing machine at a cross-head speed of 1 mm/min. The data were analysed using ANOVA and the Tukey test. The fracture surfaces were examined by optical microscopy. The bond strength of Superbond to dentine was significantly higher (P<0.05) than any of the materials tested. The bond strength of all materials tested was shown to be affected by dentine depth, except for Superbond. Fractured dentine specimens showed that the samples of Superbond are almost cohesive (>90%), and the samples of other adhesives are mostly adhesive (>70%). These results confirm that Superbond is capable of forming a bond at various dentine depths.
测定了三种粘结剂(Panavia 21、Superbond、All Bond C&B Cement和Variolink(一种双固化树脂))在不同牙本质深度的剪切粘结强度。使用500目然后800目砂纸对15颗人类完全萌出的恒牙第一和第二磨牙进行湿磨,以暴露每种测试粘结剂的表层、中层和深层牙本质。每个牙本质深度制备5个样本。使用明胶胶囊将粘结剂粘结到样本上,并在37℃的水中熟化24小时。使用拉伸试验机以1mm/min的十字头速度对样本进行剪切脱粘。使用方差分析和Tukey检验对数据进行分析。通过光学显微镜检查断裂表面。Superbond与牙本质的粘结强度显著高于(P<0.05)任何测试材料。除Superbond外,所有测试材料的粘结强度均受牙本质深度影响。断裂的牙本质标本显示,Superbond的样本几乎是内聚性的(>90%),而其他粘结剂的样本大多是粘结性的(>70%)。这些结果证实Superbond能够在不同牙本质深度形成粘结。