Suppr超能文献

不同溶液对复合树脂材料表面硬度的影响。

Effects of different solutions on the surface hardness of composite resin materials.

作者信息

Yanikoğlu Nuran, Duymuş Zeynep Yeşil, Yilmaz Baykal

机构信息

Department of Prosthodontics, School of Dentistry, Atatürk University, Erzurum, Turkey.

出版信息

Dent Mater J. 2009 May;28(3):344-51.

Abstract

In this study, the surface hardness of five light-cured composite resins were evaluated, namely: filled (Estelite), nanofil (AElite), unfilled (Valux Plus), hybrid (Tetric ceram), and Ormocer-based (Admira) composite resins. The microhardness values of composite specimens were measured at the top and bottom surfaces after 24 hours or 30 days of immersion in different solutions (tea, coffee, Turkish coffee, mouthwash, cola, and distilled water). Comparisons were made with univariate analysis of variance and Duncan's multiple range test. It was found that rough specimens of reinforced nano-hybrid composite material immersed in cola for 30 days had the lowest surface hardness (33.20), whereas rough specimens of hybrid composite material immersed in cola for 24 hours had the highest surface hardness (156.00). In both tea and coffee, the top surfaces tended to be harder than the bottom ones. In conclusion, the five different materials exhibited different hardnesses, and that the hardness values of composite materials were statistically different in different immersion solutions.

摘要

在本研究中,对五种光固化复合树脂的表面硬度进行了评估,分别为:填充型(Estelite)、纳米填料型(AElite)、未填充型(Valux Plus)、混合型(Tetric ceram)和基于Ormocer的(Admira)复合树脂。复合树脂试样在不同溶液(茶、咖啡、土耳其咖啡、漱口水、可乐和蒸馏水)中浸泡24小时或30天后,在顶面和底面测量其显微硬度值。采用单因素方差分析和邓肯多重极差检验进行比较。结果发现,浸泡在可乐中30天的增强纳米混合复合材料粗糙试样表面硬度最低(33.20),而浸泡在可乐中24小时的混合复合材料粗糙试样表面硬度最高(156.00)。在茶和咖啡中,顶面往往比底面更硬。总之,这五种不同材料表现出不同的硬度,并且复合材料在不同浸泡溶液中的硬度值在统计学上存在差异。

文献AI研究员

20分钟写一篇综述,助力文献阅读效率提升50倍。

立即体验

用中文搜PubMed

大模型驱动的PubMed中文搜索引擎

马上搜索

文档翻译

学术文献翻译模型,支持多种主流文档格式。

立即体验