Temperature-responsive phase separation of poly(N-(2-ethoxyethyl)acrylamide) (PEoEA, phase transition temperature, T(p) = 38 degrees C) and poly(N-(2-ethoxyethyl)methacrylamide) (PEoEMA, T(p) = 50 degrees C) in aqueous solutions has been investigated by infrared spectroscopy. They had a wide transition temperature region ( approximately 25 degrees C), and their T(p) monotonically increased with increasing concentration of added methanol, unlike re-entrant phase separation of poly(N-isopropylacrylamide) (PNiPAM). Their amide I bands consisted of two components assignable to singly and doubly hydrogen bonding C horizontal lineO groups in both aqueous solutions and methanol/water mixtures. The intensity of the latter decreased during both phase separation and an increase in methanol concentration, whereas the nu(C-H) bands underwent red shifts. The changes were qualitatively the same as those of PNiPAM, although PNiPAM has a higher tendency to accept double hydrogen bonds at the C horizontal lineO groups. The behavior of the copolymers of N-(2-ethoxyethyl)acrylamide and N-isopropylacrylamide in methanol/water mixtures gradually approached that of PNiPAM with an increasing content of the latter, suggesting that the interaction between each individual monomer unit and solvent molecules cooperatively determines their behavior as a whole.
通过红外光谱研究了聚(N-(2-乙氧基乙基)丙烯酰胺)(PEoEA,相变温度,T(p)=38℃)和聚(N-(2-乙氧基乙基)甲基丙烯酰胺)(PEoEMA,T(p)=50℃)在水溶液中的温度响应相分离。它们具有较宽的转变温度范围(约25℃),并且与聚(N-异丙基丙烯酰胺)(PNiPAM)的折返相分离不同,其T(p)随添加甲醇浓度的增加而单调增加。它们的酰胺I带由两种成分组成,分别可归因于水溶液和甲醇/水混合物中单个和双重氢键合的C=O基团。在相分离和甲醇浓度增加过程中,后者的强度均降低,而ν(C-H)带发生红移。尽管PNiPAM在C=O基团处接受双氢键的倾向更高,但这些变化在定性上与PNiPAM的变化相同。随着N-(2-乙氧基乙基)丙烯酰胺和N-异丙基丙烯酰胺共聚物中后者含量的增加,其在甲醇/水混合物中的行为逐渐接近PNiPAM,这表明每个单体单元与溶剂分子之间的相互作用共同决定了它们作为一个整体的行为。