The Food and Environment Research Agency, York, UK.
Food Addit Contam Part A Chem Anal Control Expo Risk Assess. 2009 Dec;26(12):1602-10. doi: 10.1080/19440040903252256.
The safety of a polyester-polyurethane can coating has been assessed using a suite of complementary analytical methods to identify and estimate the concentrations of potential chemical migrants. The polyester was based on phthalic acids and aliphatic diols. The polyisocyanate cross-linking agent was 1-isocyanato-3-isocyanatomethyl-3,5,5-trimethyl cyclohexane homopolymer (IPDI) blocked with methylethylketone oxime (MEKO) to make a one-part formulation. The overall migrate, obtained using solvent extraction of cured films, comprised almost completely of 12 cyclic and one linear polyester oligomer up to molecular weight 800 and containing up to six monomer units. These 13 oligomers covered a total of 28 isomeric forms. Other minor components detected were plasticisers and surfactants as well as impurities present in the starting materials. There was no detectable residue of either the blocked isocyanate (<0.01 microg/dm(2)) used as the starting substance or the unblocked isocyanate (<0.02 microg/dm(2)). The level of extractable IPDI was used as an indicator of the completeness of cure in experimental coatings. These studies revealed that there was an influence of time, temperature and catalyst content. Polymerisation was also influenced by the additives used and by the ageing of the wet coating formulation over several months. These studies allow parameters to be specified to ensure that commercial production coatings receive a full cure giving low migration characteristics.
已使用一系列互补的分析方法评估聚酯-聚亚安酯罐内涂料的安全性,以鉴定和估算潜在化学移行物的浓度。聚酯基于邻苯二甲酸和脂肪族二醇。多异氰酸酯交联剂为 1-异氰酸根合-3-异氰酸根合甲基-3,5,5-三甲基环己烷均聚物(IPDI),用甲乙酮肟(MEKO)封端制成单组分配方。采用固化薄膜的溶剂萃取获得的总迁移物几乎完全由 12 个环状和 1 个线性聚酯低聚物组成,分子量高达 800,含有多达 6 个单体单元。这 13 个低聚物总共涵盖了 28 种异构体形式。其他检测到的少量成分是增塑剂和表面活性剂,以及起始材料中存在的杂质。用作起始物质的封端异氰酸酯(<0.01μg/dm(2))或未封端异氰酸酯(<0.02μg/dm(2))均无检测到残留。可提取的 IPDI 水平用作实验涂层固化完全度的指标。这些研究表明,时间、温度和催化剂含量有影响。聚合还受到添加剂的影响以及湿涂层配方在数月内老化的影响。这些研究允许指定参数,以确保商业生产涂层得到充分固化,从而具有低迁移特性。