Hreniak Dariusz, Bettinelli Marco, Speghini Adolfo, Łukowiak Anna, Głuchowski Paweł, Wiglusz Rafał
Institute of Low Temperature and Structure Research, Polish Academy of Sciences, ul. Okolna 2, PL-50-422 Wroclaw, Poland.
J Nanosci Nanotechnol. 2009 Nov;9(11):6315-9. doi: 10.1166/jnn.2009.1464.
Transparent Pr-doped YAG nanoceramics composed of grains with an average size of about 42 nm, were fabricated with the Low Temperature High Pressure (LTHP) sintering technique using the corresponding nanopowders as the starting materials. The structure of the nanoceramics was analyzed by X-ray diffraction (XRD). The effect of the sintering conditions on the structural properties is discussed on the basis of the changes of the spectroscopic properties of Pr3+ ions. In particular, the intensities and decays of the emission transitions originating from the (3)P0 and (1)D2 levels are investigated and correlated with structural properties of the material, such as microstrains produced by the high-pressure process.
采用低温高压(LTHP)烧结技术,以相应的纳米粉末为起始原料,制备了平均晶粒尺寸约为42nm的透明掺镨钇铝石榴石纳米陶瓷。通过X射线衍射(XRD)分析了纳米陶瓷的结构。基于Pr3+离子光谱性质的变化,讨论了烧结条件对结构性能的影响。特别研究了源自(3)P0和(1)D2能级的发射跃迁的强度和衰减,并将其与材料的结构性能相关联,例如高压过程产生的微应变。