牙本质粘结剂对人牙髓中 P 物质释放的影响。

The effect of dentine-bonding agents on substance P release in human dental pulp.

机构信息

Endodontic Department, School of Dentistry, Pontificia Universidad Javeriana, Bogota, Colombia.

出版信息

Int Endod J. 2010 Feb;43(2):95-101. doi: 10.1111/j.1365-2591.2009.01646.x.

Abstract

AIM

To quantify the effect of dentine-bonding agents on Substance P (SP) release in healthy human dental pulp tissue.

METHODOLOGY

Forty pulp samples were obtained from healthy pre-molars where extraction was indicated for orthodontic reasons. In thirty of these pre-molars, a standardized Class V cavity preparation was performed, and teeth were divided equally into three groups: (i) Unetched-cavity control group: Class V cavities only; (ii) Experimental Group I: 'One-step' self-etch bonding agent was placed in the cavity; and (iii) Experimental Group II: 'Two-step' total-etch bonding agent was placed in the cavity. The remaining ten healthy pre-molars where extracted without treatment and served as an intact-teeth control group. SP was measured by radioimmunoassay.

RESULTS

Greater SP release was found in the 'one-step' bonding agent group, followed by the 'two-step' bonding agent group and the unetched-cavity control group. The lower SP values were for the intact-teeth control group. anova showed statistically significant differences between groups (P = 0.0001). Tukey HSD post hoc tests showed statistically significant differences in SP release between the intact-teeth control group and the three other groups (P < 0.01) and between the unetched-cavity control group and the 'one-step' bonding agent group (P < 0.05). No significant difference was found between the 'two-step' bonding agent and the unetched-cavity control group.

CONCLUSION

Dentine-bonding agents placed over Class V cavity preparations increased SP release. One-step dentine-bonding agents increased SP release most.

摘要

目的

定量研究牙本质粘结剂对健康人牙髓组织中 P 物质(SP)释放的影响。

方法

从因正畸需要拔除的健康前磨牙中获取 40 个牙髓样本。在其中 30 个前磨牙上进行标准化的 V 类洞制备,并将牙齿平均分为三组:(i)未蚀刻窝洞对照组:仅制备 V 类窝洞;(ii)实验组 I:“一步法”自酸蚀粘结剂置于窝洞内;(iii)实验组 II:“两步法”全酸蚀粘结剂置于窝洞内。其余 10 个健康前磨牙未经处理作为完整牙对照组。通过放射免疫分析法测量 SP。

结果

“一步法”粘结剂组的 SP 释放量最大,其次是“两步法”粘结剂组和未蚀刻窝洞对照组。完整牙对照组的 SP 值较低。方差分析显示各组间差异具有统计学意义(P = 0.0001)。Tukey HSD 事后检验显示,完整牙对照组与其他三组之间的 SP 释放差异具有统计学意义(P < 0.01),未蚀刻窝洞对照组与“一步法”粘结剂组之间的差异也具有统计学意义(P < 0.05)。“两步法”粘结剂组与未蚀刻窝洞对照组之间无显著差异。

结论

置于 V 类窝洞预备体上的牙本质粘结剂增加了 SP 的释放。“一步法”牙本质粘结剂增加 SP 释放最多。