Vavken Patrick, Joshi Shilpa M, Murray Martha M
Department of Orthopedic Surgery, Children's Hospital Boston, Harvard Medical School, Boston, MA, USA.
Knee. 2011 Jan;18(1):42-6. doi: 10.1016/j.knee.2009.12.008. Epub 2010 Jan 18.
Fibrin is a frequently used biomaterial in surgery and tissue engineering. While it has been shown that fibrin supports cellular proliferation and biosynthesis, there is a scarcity of studies focusing on the effects of fibrin concentration. The objective of this study is to assess the effect of fibrin concentrations around the physiological concentration of 3mg/ml on the behavior of ligament fibroblasts. Fibroblasts were obtained from the anterior cruciate ligaments of four pigs and seeded throughout fibrin gels of either 1, 3, or 6 mg/ml fibrin. The gels were collected at 2, 6, and 10 days for measurement of DNA and collagen content. We found that both DNA and collagen content increased significantly over time in gels made with all concentrations of fibrin. However, the increases were significantly lower in gels made with the higher concentrations of fibrin (3 and 6 mg/ml). Microscopic assessment of FITC-labeled gels showed a decrease in pore size at high fibrin concentrations, which might be a reason for the observed effect on bioactivity. To enhance cell behavior and thus clinical results fibrin applications should build on physiologic or sub-physiologic concentrations, and those with higher concentrations, such as currently available sealants, should be used cautiously.
纤维蛋白是外科手术和组织工程中常用的生物材料。虽然已经表明纤维蛋白支持细胞增殖和生物合成,但专注于纤维蛋白浓度影响的研究却很匮乏。本研究的目的是评估在生理浓度3mg/ml左右的纤维蛋白浓度对韧带成纤维细胞行为的影响。从四只猪的前交叉韧带中获取成纤维细胞,并接种到纤维蛋白浓度为1mg/ml、3mg/ml或6mg/ml的纤维蛋白凝胶中。在第2天、第6天和第10天收集凝胶,用于测量DNA和胶原蛋白含量。我们发现,在所有浓度纤维蛋白制成的凝胶中,DNA和胶原蛋白含量均随时间显著增加。然而,在较高浓度(3mg/ml和6mg/ml)纤维蛋白制成的凝胶中,增加幅度明显较低。对异硫氰酸荧光素标记凝胶的显微镜评估显示,高纤维蛋白浓度下孔径减小,这可能是观察到的对生物活性产生影响的一个原因。为了增强细胞行为从而改善临床结果,纤维蛋白的应用应以生理或亚生理浓度为基础,而对于那些较高浓度的产品,如目前可用的密封剂,应谨慎使用。