基于低聚合收缩硅氧烷的复合材料的边缘适合性:1 年随机临床试验。

Marginal adaptation of a low-shrinkage silorane-based composite: 1-year randomized clinical trial.

机构信息

Department of Pediatric Dentistry, School of Dentistry, Faculty of Health Sciences, Århus University, Århus, Denmark.

出版信息

Clin Oral Investig. 2011 Apr;15(2):291-5. doi: 10.1007/s00784-010-0446-2. Epub 2010 Jul 20.

Abstract

The aim of the present study was to examine the marginal adaptation of a new low-shrinkage silorane-based composite material (Filtek™ Silorane, 3M-Espe) by comparing it with a methacrylate-based composite material (CeramX™, Dentsply DeTrey). In particular, we wanted to test the hypothesis that reduced polymerization shrinkage would improve the marginal adaptation. Seventy-two patients participated in the study. A total of 158 restorations were placed in 80 premolars and 78 molars. Only Class II restorations were included, and each patient could contribute with more than one tooth. The restorations were scored at baseline and after one year. While statistical comparison of marginal adaptation at follow-up indicated better performance of CeramX™ both occlusally and approximally (p = 0.01 and p < 0.01), the low kappa value (32%) reflects the difficulty to assess marginal adaptation clinically. The reduction in polymerization shrinkage demonstrated in the laboratory was not clinically significant in the present study.

摘要

本研究旨在通过比较新型低收缩硅烷基复合材料(Filtek™ Silorane,3M-Espe)与甲基丙烯酸酯基复合材料(CeramX™,Dentsply DeTrey),来检测其边缘适合性。具体而言,我们想要验证一个假设,即降低聚合收缩率将改善边缘适应性。72 名患者参与了本研究。共在 80 颗前磨牙和 78 颗磨牙上放置了 158 个修复体。仅纳入 II 类修复体,每位患者可贡献一颗以上的牙齿。在基线和一年后对修复体进行评分。虽然在随访时对边缘适应性的统计学比较表明 CeramX™在近远中面的性能更好(p = 0.01 和 p < 0.01),但低kappa 值(32%)反映了临床上评估边缘适应性的难度。本研究中,实验室中显示的聚合收缩减少在临床上并不显著。