Soh G, Chew C L, Lee A S, Yeoh T S
National University of Singapore.
Quintessence Int. 1991 Mar;22(3):225-8.
The potential risks of mercury dissolution from dental amalgam have long been recognized. This study examined the effect of hydrogen ion concentration on the release of mercury from two dental amalgams: an admixed high-copper amalgam and a new tin- and copper-free amalgam. Specimens of each type of amalgam were incubated citric acid buffer of pH 2.5 or pH 7.0. Results showed that, for both types of amalgam, specimens incubated at pH 2.5 released statistically significantly greater (P less than .0001) quantities of mercury than did specimens incubated at pH 7.0. Release of mercury from the tin- and copper-free amalgam was also statistically significantly greater (P less than .0001) than that of the higher-copper amalgam at both pH levels.
牙科汞合金中汞溶解的潜在风险早已为人所知。本研究考察了氢离子浓度对两种牙科汞合金汞释放的影响:一种是混合型高铜汞合金,另一种是新型无锡无铜汞合金。每种汞合金的样本在pH值为2.5或pH值为7.0的柠檬酸缓冲液中孵育。结果显示,对于这两种汞合金,在pH值为2.5下孵育的样本释放的汞量在统计学上显著高于(P小于0.0001)在pH值为7.0下孵育的样本。在两个pH水平下,无锡无铜汞合金的汞释放量在统计学上也显著高于(P小于0.0001)高铜汞合金。