Abstract

Conditioning of the enamel surface is now an accepted and widely applied technique used to improve retention in porcelain laminate veneer restorations. The aim of this study was to evaluate strength of the bond between porcelain laminate veneers and tooth surfaces etched with acid and laser, separately and together. The teeth studied comprised 60 incisors extracted for periodontal reasons. These were divided into four groups according to etching method: group 1, acid etching alone; group 2, acid etching followed by laser etching; group 3, laser etching followed by acid etching; group 4, laser etching alone. The teeth were etched with 37% phosphoric acid and a Er,Cr:YSGG laser system. In addition, 60 IPS Empress II cylindrical blocks 2 mm in height and 5 mm in diameter were also prepared for the etched tooth surface. These blocks were bonded to the teeth with dual cured resin cement and shear tests were then performed. After the shear tests, Scanning electron microscopy images of the tooth surfaces were obtained at a magnification of ×3,800. Etching with acid alone yielded the highest mean value of bond shear strength (15.4±3.8 MPa), while laser etching followed by acid etching gave the lowest mean value (11.5±4.6 MPa). The mean values of the bond shear strength for acid etching followed by laser etching and laser etching alone were 13.8±3.9 MPa and 12.8±4.6 MPa, respectively. Statistical analysis revealed no significant differences between the groups. The results suggest that laser etching is easy to apply and less time-consuming. They further suggest that the order in which the acid and laser are applied in combined treatments is important.

摘要

牙釉质表面处理现已被广泛接受并应用于瓷贴面修复体,以提高其固位力。本研究旨在评估酸蚀和激光单独及联合处理后瓷贴面与牙面之间的粘结强度。研究对象为 60 颗因牙周原因拔除的切牙,根据酸蚀方法将其分为 4 组:组 1,单独酸蚀;组 2,酸蚀后激光蚀刻;组 3,激光蚀刻后酸蚀;组 4,单独激光蚀刻。牙齿用 37%磷酸酸蚀和 Er,Cr:YSGG 激光系统处理。此外,还制备了 60 个高度 2mm、直径 5mm 的 IPS Empress II 圆柱块用于处理牙面。这些块体用双固化树脂水门汀粘结到牙齿上,然后进行剪切试验。剪切试验后,用扫描电子显微镜在 ×3800 放大倍数下观察牙面。单独酸蚀的粘结剪切强度平均值最高(15.4±3.8 MPa),而激光蚀刻后酸蚀的平均值最低(11.5±4.6 MPa)。酸蚀后激光蚀刻和单独激光蚀刻的粘结剪切强度平均值分别为 13.8±3.9 MPa 和 12.8±4.6 MPa。统计学分析显示各组间无显著差异。结果表明激光蚀刻易于操作且耗时较少。进一步表明在联合治疗中酸蚀和激光的应用顺序很重要。