Garcia-Godoy F, Olsen B T, Marshall T D, Barnwell G M
University of Texas Health Science Center at San Antonio.
Am J Dent. 1990 Jun;3(3):94-6.
This study evaluated the amount of fluoride released from amalgam restorations lined with a silver-reinforced glass ionomer. Thirty human extracted molars were divided into three groups of 10 teeth each. Group 1: Class V cavities were made on the facial surfaces and restored with Dispersalloy amalgam. Group 2: Same as Group 1 except 1 mm of GC Lining glass ionomer cement (GIC) was placed on the axial wall before amalgam insertion. Group 3: Same as Group 2 except 1 mm of Miracle Mix silver-reinforced glass ionomer cement (GIC) was placed on the axial wall before amalgam insertion. Before any treatment, all samples were placed in polyethylene vials with 4 ml of deionized water and thermocycled (100x) for baseline fluoride release levels. After restoration, each tooth was replaced in a vial with 4 ml of deionized water. At weekly intervals, each tooth was removed from its aqueous medium and transferred to another vial containing 4 ml of deionized water. Fluoride release was measured four times at weekly intervals with an Orion #9609 fluoride-ion electrode. At 1 and 4 weeks, Miracle Mix released significantly more fluoride than GC Lining (P less than 0.0001).
本研究评估了衬有银增强玻璃离子体的汞合金修复体释放氟化物的量。30颗拔除的人类磨牙被分为三组,每组10颗牙齿。第1组:在颊面制备V类洞,并用Dispersalloy汞合金修复。第2组:与第1组相同,只是在汞合金充填前在轴壁上放置1mm的GC Lining玻璃离子水门汀(GIC)。第3组:与第2组相同,只是在汞合金充填前在轴壁上放置1mm的Miracle Mix银增强玻璃离子水门汀(GIC)。在任何治疗前,将所有样本置于装有4ml去离子水的聚乙烯小瓶中,并进行热循环(100次)以测定基线氟化物释放水平。修复后,将每颗牙齿放回装有4ml去离子水的小瓶中。每周一次,将每颗牙齿从其水性介质中取出,并转移到另一个装有4ml去离子水的小瓶中。使用Orion #9609氟离子电极每周测量四次氟化物释放量。在第1周和第4周,Miracle Mix释放的氟化物明显多于GC Lining(P小于0.0001)。