Suppr超能文献

大尺寸粘接性 IV 类复合树脂修复体在人工老化前后的边缘适合性。

Marginal adaptation of large adhesive class IV composite restorations before and after artificial aging.

机构信息

University of Geneva, Geneva, Switzerland.

出版信息

J Adhes Dent. 2011 Oct;13(5):425-31. doi: 10.3290/j.jad.a19649.

Abstract

PURPOSE

To test the marginal adaptation of Class IV restorations made of different composite materials designed for anterior use.

MATERIALS AND METHODS

Forty-two extracted caries-free human maxillary central incisors were randomly divided into 7 experimental groups - one per composite tested - for which Class IV cavities were prepared. The microfilled composite materials tested (SolidBond/Durafill [D/SB], Syntac classic/Heliomolar [H/SC], Scotchbond1/ Experiment127 [EXI/SB1], Optibond FL/Point 4 [P4/OBFL], Prime&Bond NT/Esthet-X [EX/PBNT], ART Bond/ Miris [MIR/ART], SE Bond/Clearfil ST [CLE/SE-B]) were inserted in two increments after polymerization of their respective adhesive systems. While under simulated dentinal fluid pressure, specimens were submitted to cyclic incisal stress (1,200,000 cycles, maximum load 49 N) and thermal loading (3000 cycles). Both after polishing and after thermomechanical loading, impressions were made of the surface of each restoration, and epoxy replicas were prepared for the marginal adaptation evaluation using SEM.

RESULTS

Perfect margins before loading in enamel ranged from 49.9% (EXI/SB1) to 98.2% (MIR/ART) and after loading from 25.3% (EXI/SB1) to 91.9% (MIR/ART). For margins located in dentin, perfect margins ranged from 16.8% (EXI/SB1) to 100% (CLE/SE-B) before loading and from 4.6% (EXI/SB1) to 67.1% (CLE/SE-B) after loading.

CONCLUSION

The poor results obtained in this in-vitro test with the microfilled composites suggest avoiding their use in large Class IV restorations with margins in dentin.

摘要

目的

测试用于前牙的不同复合树脂材料制成的 IV 类修复体的边缘适应性。

材料和方法

将 42 颗无龋的上颌中切牙随机分为 7 个实验组-每个实验组测试一种复合树脂-制备 IV 类洞型。测试的微填充复合树脂材料(SolidBond/Durafill [D/SB]、Syntac classic/Heliomolar [H/SC]、Scotchbond1/Experiment127 [EXI/SB1]、Optibond FL/Point 4 [P4/OBFL]、Prime&Bond NT/Esthet-X [EX/PBNT]、ART Bond/Miris [MIR/ART]、SE Bond/Clearfil ST [CLE/SE-B])在各自的粘接系统聚合后分两次填入。在模拟牙本质液压力下,试件在 49N 的最大载荷下进行 120 万次的牙尖交错位循环加载和热加载。抛光后和热机械加载后,对每个修复体表面进行印模,并用 SEM 制备用于边缘适应性评估的环氧复制件。

结果

在釉质加载前的完美边缘比例从 49.9%(EXI/SB1)到 98.2%(MIR/ART),加载后从 25.3%(EXI/SB1)到 91.9%(MIR/ART)。对于位于牙本质的边缘,在加载前完美边缘比例从 16.8%(EXI/SB1)到 100%(CLE/SE-B),加载后从 4.6%(EXI/SB1)到 67.1%(CLE/SE-B)。

结论

这项体外试验中微填充复合树脂的结果较差,建议避免在位于牙本质的大的 IV 类修复体中使用。