Joseph Lori A, Israel Omoniyi K, Edet Ekanem J
PhD of Chemistry, Department of Chemistry, Ahmadu Bello University, Zaria, Nigeria.
Dent Res J (Isfahan). 2009 Spring;6(1):7-11.
The study was designed to investigate the effects of pH, chloride ions and nature of some bio-fluids on the amount of metal ions released from titanium and TiAl(6)Nb(7) plates following incubation in actual and simulated bio-fluids over time.
The amounts of released metal ions from commercially pure titanium (CpTi) and TiAl(6)Nb(7)of surgical grade on immersion in 20 mL Hank's solution of pH 4.0 or 7.0, Hank's solution of high chloride ions concentration, Whole Blood Serum (WBS) and Phosphate Buffered Saline (PBS) at 37° C were determined over an incubation time of 20 weeks using atomic absorption spectrophotometry. The levels of released metal ions were compared by two-way ANOVA and Duncan's post-hoc tests. The amounts of titanium ions released by the samples were analyzed by Pearson's correlation.
TiAl(6)Nb(7) plate showed no release of Ti ions into the test solutions until after 12 weeks of incubation, while Ti ions were released from the CpTi plate from the 1 day immersion time. The release of measurable amount of Al ions from TiAl(6)Nb(7)was after 12 weeks of incubation. The rate of release of Ti and Al ions from the samples increased initially with incubation time and then stabilized due to adsorption-desorption equilibrium.
The results showed that variations in pH and chloride ions of the test media has a significant effect on the amounts of Ti ions released, while increase in chloride ions concentration significantly elevates the release of Al ions into the biofluids.
本研究旨在调查pH值、氯离子以及某些生物流体的性质对钛板和TiAl(6)Nb(7)板在实际和模拟生物流体中孵育一段时间后释放的金属离子量的影响。
使用原子吸收分光光度法,在37℃下,将商业纯钛(CpTi)和外科级TiAl(6)Nb(7)浸入20 mL pH值为4.0或7.0的汉克溶液、高氯离子浓度的汉克溶液、全血血清(WBS)和磷酸盐缓冲盐水(PBS)中20周,测定释放的金属离子量。通过双向方差分析和邓肯事后检验比较释放的金属离子水平。通过皮尔逊相关性分析样品释放的钛离子量。
TiAl(6)Nb(7)板在孵育12周后才开始向测试溶液中释放Ti离子,而CpTi板在浸入1天后就开始释放Ti离子。TiAl(6)Nb(7)在孵育12周后开始释放可测量量的Al离子。样品中Ti和Al离子的释放速率最初随孵育时间增加,然后由于吸附 - 解吸平衡而稳定。
结果表明,测试介质的pH值和氯离子变化对释放的Ti离子量有显著影响,而氯离子浓度的增加显著提高了Al离子向生物流体中的释放量。