Department of Restorative Dentistry, Piracicaba Dental School, State University of Campinas, Piracicaba, SP, Brazil.
Braz Oral Res. 2011 Mar-Apr;25(2):168-73. doi: 10.1590/s1806-83242011000200012.
The aim of this in vitro study was to evaluate the effect of different mouthwashes on superficial roughness and Knoop hardness of two resin composites. Eighty specimens (6 mm Ø and 2 mm height) were prepared and divided into eight experimental groups (n = 10) according to the resin composites (4 Seasons and Esthet X), and storage solutions (G1 - Distilled water; G2 - Colgate Plax Overnight; G3 - Colgate Plax Alcohol Free; and G4 - Colgate Plax Whitening). The initial hardness and roughness readings (T1) were measured and then the specimens were stored in 2 mL of mouthwash for 12 h (T2) and 24 h (T3). The data were analyzed with repeat-measures two-way ANOVA and Tukey's test (α = 5%). Regardless of the type of solution and time of exposure, there was no statistical difference for roughness between the resins (p = 0.44). G4 and G8 presented higher roughness means than G1, G3, G5 and G7, after 12 and 24 hours of immersion. For Knoop microhardness analysis, there was a significant reduction for all groups after 12 hours and 24 hours. We conclude that the mouthwashes containing hydrogen peroxide and/or alcohol decrease the microhardness of the resins tested; however, the mouthwash containing hydrogen peroxide had a higher deleterious effect on roughness.
本体外研究旨在评估不同漱口水对两种树脂复合材料表面粗糙度和努氏硬度的影响。将 80 个试件(直径 6mm,高度 2mm)根据树脂复合材料(4 Seasons 和 Esthet X)和储存溶液(G1-蒸馏水;G2-Colgate Plax 隔夜;G3-Colgate Plax 无酒精;G4-Colgate Plax 美白)分为 8 个实验组(n=10)。测量初始硬度和粗糙度读数(T1),然后将试件储存在 2mL 漱口水 12 小时(T2)和 24 小时(T3)。使用重复测量双向方差分析和 Tukey 检验(α=5%)对数据进行分析。无论溶液类型和暴露时间如何,两种树脂之间的粗糙度均无统计学差异(p=0.44)。G4 和 G8 在浸泡 12 小时和 24 小时后,其粗糙度均值均高于 G1、G3、G5 和 G7。对于努氏硬度分析,所有组在 12 小时和 24 小时后均显著降低。我们得出结论,含过氧化氢和/或酒精的漱口水会降低所测试的树脂的显微硬度;然而,含过氧化氢的漱口水对粗糙度的有害影响更大。