体外评估新型美学复合树脂对不同背景的分光光度性能。

Spectrophotometric evaluation of a novel aesthetic composite resin with respect to different backgrounds in vitro.

机构信息

Department of Operative Dentistry, University of Marburg, Georg-Voigt-Strasse 3, Marburg, Germany.

出版信息

Odontology. 2013 Jan;101(1):60-6. doi: 10.1007/s10266-011-0055-9. Epub 2011 Dec 30.

Abstract

Tooth colour matching of composite materials is often a common problem caused by a dark background from the oral cavity. Therefore, the aim of the study was to evaluate a novel aesthetic composite material and to assess the influence of white and black backgrounds. Tooth shades of 30 freshly extracted upper front teeth were determined using a spectrophotometer (SpectroShade™) both against a white and a black background. Two class IV cavities in each tooth were prepared and restored using three different composite resins: Arabesk™ (AB), Synergy™ (SE) and the novel material Amaris™ (AM). After water storage for 1 week, differences in hue, saturation and lightness were measured to assess changes from baseline. After thermocycling, teeth were evaluated once more to assess the reliability of the treatment outcomes. Compared to baseline, differences in hue were not statistically different for all restoration materials (p > 0.05) with respect to the white or black background. Delta values for saturation were not different in the AB and AM groups (p > 0.05) with higher values for SE (p < 0.05). Regarding lightness, values in the AB group were statistically higher (p < 0.05) than values for AM with no difference between AB and SE and with no difference between the AM and SE groups (p > 0.05). Employing the novel aesthetic composite resin, a minor impact of white and black backgrounds could be observed compared to conventional composites. Therefore, it might effectively mask the dark background from the oral cavity.

摘要

复合材料的牙齿颜色匹配常常是由口腔内深色背景引起的常见问题。因此,本研究的目的是评估一种新型美学复合材料,并评估白色和黑色背景的影响。使用分光光度计(SpectroShade™)分别在白色和黑色背景下对 30 颗刚拔出的上颌前牙的牙色进行了测定。在每颗牙上制备两个 IV 类洞,并使用三种不同的复合树脂进行修复:Arabesk™(AB)、Synergy™(SE)和新型材料 Amaris™(AM)。水储存 1 周后,测量色调、饱和度和明度的差异,以评估从基线的变化。冷热循环后,再次评估牙齿,以评估治疗效果的可靠性。与基线相比,所有修复材料在白色或黑色背景下的色调差异均无统计学意义(p>0.05)。AB 和 AM 组的饱和度差值没有差异(p>0.05),而 SE 组的饱和度差值较高(p<0.05)。关于明度,AB 组的值明显高于 AM 组(p<0.05),AB 组与 SE 组之间无差异,AB 组与 SE 组之间也无差异(p>0.05)。与传统复合材料相比,新型美学复合树脂对白色和黑色背景的影响较小。因此,它可能有效地掩盖口腔内的深色背景。

文献检索

告别复杂PubMed语法,用中文像聊天一样搜索,搜遍4000万医学文献。AI智能推荐,让科研检索更轻松。

立即免费搜索

文件翻译

保留排版,准确专业,支持PDF/Word/PPT等文件格式,支持 12+语言互译。

免费翻译文档

深度研究

AI帮你快速写综述,25分钟生成高质量综述,智能提取关键信息,辅助科研写作。

立即免费体验