往复运动镍钛器械 Reciproc 和 WaveOne 的疲劳寿命。

Cyclic fatigue of Reciproc and WaveOne reciprocating instruments.

机构信息

Department of Endodontics, Sapienza University of Rome, Via Tommaso Salvini 57, Rome, Italy.

出版信息

Int Endod J. 2012 Jul;45(7):614-8. doi: 10.1111/j.1365-2591.2012.02015.x. Epub 2012 Jan 23.

Abstract

AIM

To evaluate the cyclic fatigue resistance of Reciproc(®) and WaveOne(®) instruments in simulated root canals.

METHODOLOGY

Two groups of 15 NiTi endodontic instruments of identical tip size of 0.25 mm were tested, group A; Reciproc(®) R25 and group B: WaveOne(®) primary. Cyclic fatigue testing was performed in a stainless steel artificial canal manufactured by reproducing the instrument's size and taper. A simulated root canal with a 60° angle of curvature and 5-mm radius of curvature was constructed for both the instruments tested. The centre of the curvature was 5 mm from the tip of the instrument and the curved segment of the canal was approximately 5 mm in length. The Reciproc(®) instruments were activated using the preset programme specific for the Reciproc(®) instruments, whilst the WaveOne(®) instruments were activated using the preset programme specific for the WaveOne(®) instruments. All instruments were rotated until fracture occurred and the time to fracture (TtF) and the length of the fractured tip were recorded and registered. Means and standard deviations of TtF and fragment length were calculated for each system and data were subjected to Student's t-test (P < 0.05).

RESULTS

A statistically significant difference (P < 0.05) was noted between Reciproc(®) and WaveOne(®) instruments. Reciproc(®) R25 instruments were associated with a significant increase in the mean time to fracture when compared with primary WaveOne(®) instruments (130.8 ± 18.4 vs. 97.8 ± 15.9 s). There was no significant difference (P > 0.05) in the mean length of the fractured fragments between the instruments.

CONCLUSIONS

Reciproc(®) instruments were associated with a significantly higher cyclic fatigue resistance than WaveOne(®) instruments.

摘要

目的

评估 Reciproc(®)和 WaveOne(®)仪器在模拟根管中的抗循环疲劳性能。

方法

测试了两组相同尖端尺寸为 0.25mm 的 15 根镍钛根管器械,组 A:Reciproc(®)R25 和组 B:WaveOne(®)初级。循环疲劳测试在由复制器械尺寸和锥度制成的不锈钢人工管中进行。为两种测试仪器构建了一个具有 60°曲率角和 5mm 曲率半径的模拟根管。曲率中心距器械尖端 5mm,弯曲段约 5mm 长。Reciproc(®)仪器使用特定于 Reciproc(®)仪器的预设程序激活,而 WaveOne(®)仪器使用特定于 WaveOne(®)仪器的预设程序激活。所有仪器均旋转至断裂发生,并记录和注册断裂时间(TtF)和断裂尖端的长度。计算了每个系统的 TtF 和片段长度的平均值和标准偏差,并对数据进行了学生 t 检验(P<0.05)。

结果

Reciproc(®)和 WaveOne(®)仪器之间存在统计学显著差异(P<0.05)。与初级 WaveOne(®)仪器相比,Reciproc(®)R25 仪器的平均断裂时间显著增加(130.8±18.4 与 97.8±15.9 s)。仪器断裂碎片的平均长度之间无显著差异(P>0.05)。

结论

Reciproc(®)仪器的抗循环疲劳性能明显高于 WaveOne(®)仪器。