Angle Orthod. 2012 Nov;82(6):1071-7. doi: 10.2319/101711-644.1. Epub 2012 Mar 22.
To evaluate in vitro the influence of topical fluoride application on the mechanical properties of orthodontic cements containing fluoride under pH cycling conditions.
Edgewise brackets for maxillary central incisors were bonded to 192 bovine incisors using Transbond XT (G1), Transbond Plus Color Change (G2), and Fuji Ortho LC (G3) (n = 64 for each group). The specimens of each group were subdivided (n = 16) into different subgroups. Subgroup A received no topical fluoride application during pH cycling, while the experimental subgroups received topical fluoride treatments as follows: B, application three times per day of fluoride dentifrice (1450 ppm F); C, application one time per day of fluoride mouth rinse (250 ppm F); and D, combination of fluoride dentifrice and fluoride mouth rinse. After 14 days of pH cycling, the shear bond strength and Adhesive Remnant Index were evaluated statistically.
Polarized light microscopy showed that pH cycling induced mineral loss in all specimens. The topical application of fluoride did not have an influence on shear bond strength, although the association of fluoride dentifrice and mouth rinse increased the shear bond strength of the resinous cement without fluoride (P < .01). Regarding the Adhesive Remnant Index, no statistical differences were found within the groups G1 (P = .23), G2 (P = .47), and G3 (P = .74).
Topical fluoride treatments improved the shear bond strength of resinous cement, regardless of the material's fluoride-releasing capacity, and reached the adhesive fractures.
评估在 pH 循环条件下,局部应用氟化物对含氟正畸粘接剂的机械性能的体外影响。
使用 Transbond XT(G1)、Transbond Plus Color Change(G2)和 Fuji Ortho LC(G3)将上颌中切牙的方丝弓托槽粘接到 192 颗牛切牙上(每组 n = 64)。将每组的标本(n = 16)进一步分为不同亚组。亚组 A 在 pH 循环期间未接受局部氟化物处理,而实验组亚组接受以下局部氟化物处理:B,每天三次应用含氟牙膏(1450 ppm F);C,每天一次应用含氟漱口水(250 ppm F);D,含氟牙膏和含氟漱口水联合应用。在 pH 循环 14 天后,对剪切粘结强度和粘固剂残留指数进行统计学评估。
偏光显微镜显示,pH 循环导致所有标本的矿物质损失。局部应用氟化物对接合力强度没有影响,尽管氟化物牙膏和漱口水的联合应用增加了不含氟的树脂粘结剂的剪切粘结强度(P <.01)。关于粘固剂残留指数,G1 组(P = .23)、G2 组(P = .47)和 G3 组(P = .74)内均无统计学差异。
局部氟化物处理改善了树脂粘结剂的剪切粘结强度,无论材料的释氟能力如何,都能达到粘结剂断裂。