Laser Research Center of Dentistry (LRCD), Dental Materials Department, Tehran University of Medical Sciences, Tehran, Iran.
Lasers Med Sci. 2013 Jan;28(1):139-42. doi: 10.1007/s10103-012-1086-3. Epub 2012 Apr 11.
The purpose of this study was to evaluate the effect of Er:YAG and Er,Cr:YSGG laser on tensile bond strength of composite resin to dentine in comparison with bur-prepared cavities. Fifteen extracted caries-free human third molars were selected. The teeth were cut at a level below the occlusal pit and fissure plan and randomly divided into three groups. Five cavities were prepared by diamond bur, five cavities prepared by Er:YAG laser, and the other group prepared by Er,Cr:YSGG laser. Then, all the cavities were restored by composite resin. The teeth were sectioned longitudinally with Isomet and the specimens prepared in dumbbelled shape (n = 36). The samples were attached to special jigs, and the tensile bond strength of the three groups was measured by universal testing machine at a speed of 0.5 mm/min. The results of the three groups were analyzed with one-way ANOVA and Tamhane test. The means and standard deviations of tensile bond strength of bur-cut, Er:YAG laser-ablated, and Er,Cr:YSGG laser-ablated dentine were 5.04 ± 0.93, 13.37 ± 3.87, and 4.85 ± 0.93 MPa, respectively. There is little difference in tensile bond strength of composite resin in Er,Cr:YSGG lased-prepared cavities in comparison with bur-prepared cavities, but the Er:YAG laser group showed higher bond strength than the other groups.
本研究旨在评估 Er:YAG 和 Er,Cr:YSGG 激光对牙本质与复合树脂间拉伸粘结强度的影响,并与车针预备的窝洞进行比较。选取 15 颗无龋的人第三磨牙,于咬合面下窝沟水平切割,随机分为三组。每组 5 个窝洞,一组由钻石车针预备,一组由 Er:YAG 激光预备,另一组由 Er,Cr:YSGG 激光预备。然后用复合树脂修复所有窝洞。用 Isomet 沿牙体长轴将牙齿纵向劈开,制备哑铃形试件(n = 36)。将试件固定在专用夹具上,以 0.5mm/min 的速度用万能试验机测量三组的拉伸粘结强度。采用单因素方差分析和 Tamhane 检验对三组结果进行分析。车针预备、Er:YAG 激光预备和 Er,Cr:YSGG 激光预备牙本质的复合树脂拉伸粘结强度均值和标准差分别为 5.04 ± 0.93、13.37 ± 3.87 和 4.85 ± 0.93 MPa。Er,Cr:YSGG 激光预备组与车针预备组相比,复合树脂的拉伸粘结强度差异无统计学意义,但 Er:YAG 激光组的粘结强度高于其他两组。