Suppr超能文献

正畸临时锚定装置的腐蚀。

Corrosion of orthodontic temporary anchorage devices.

机构信息

Departments of Developmental Sciences/Orthodontics, Marquette University School of Dentistry, Milwaukee, WI 53201, USA

出版信息

Eur J Orthod. 2013 Aug;35(4):500-6. doi: 10.1093/ejo/cjs027. Epub 2012 May 9.

Abstract

Corrosion of orthodontic miniscrews or temporary anchorage devices (TADs) has been proposed as a contributor to inflammation, which in turn is a factor in the clinical success of miniscrews. The purpose of this study was to measure the electrochemical properties of orthodontic miniscrews in artificial saliva with and without fluoride. The corrosion properties of three miniscrew products (VectorTAS, Ormco Corp.; Unitek TAD, 3M Unitek; and Through-Hole Screw, American Orthodontics) were tested in an artificial saliva (Fusayama-Meyer) with (1500 ppm) or without fluoride (n = 10/product/solution). Open circuit potential (OCP), polarization resistance (R p), and corrosion current (I corr) were measured and statistically analysed with the Friedman/Tukey least significant difference tests. No significant differences (P > 0.05) between miniscrews with regard to OCP, R p, and I corr were found except that the American Orthodontics miniscrews had a significantly (P < 0.05) more noble OCP compared to the others. Incorporation of 1500 ppm fluoride in the artificial saliva significantly (P < 0.001) lowered the OCP, reduced the polarization resistance, and increased the corrosion current of each miniscrew product. Few differences existed in the electrochemical properties of miniscrews from the three different manufacturers; however, exposure to fluoride was detrimental to the corrosion properties of all miniscrews.

摘要

正畸微螺钉或临时锚定装置(TAD)的腐蚀被认为是炎症的一个因素,而炎症反过来又是微螺钉临床成功的一个因素。本研究的目的是测量含有和不含有氟化物的人工唾液中正畸微螺钉的电化学性能。三种微螺钉产品(VectorTAS,Ormco 公司;Unitek TAD,3M Unitek;和 Through-Hole Screw,American Orthodontics)的腐蚀性能在人工唾液(Fusayama-Meyer)中进行了测试,其中含有(1500ppm)或不含有氟化物(n=10/产品/溶液)。测量开路电位(OCP)、极化电阻(Rp)和腐蚀电流(Icorr),并用 Friedman/Tukey 最小显著差异检验进行统计学分析。除了 American Orthodontics 微螺钉的 OCP 明显(P<0.05)比其他微螺钉更正,在 OCP、Rp 和 Icorr 方面,微螺钉之间没有显著差异(P>0.05)。人工唾液中加入 1500ppm 的氟化物显著(P<0.001)降低了 OCP,降低了极化电阻,增加了每种微螺钉产品的腐蚀电流。来自三个不同制造商的微螺钉在电化学性能方面存在一些差异;然而,暴露于氟化物对所有微螺钉的腐蚀性能都有害。

文献AI研究员

20分钟写一篇综述,助力文献阅读效率提升50倍。

立即体验

用中文搜PubMed

大模型驱动的PubMed中文搜索引擎

马上搜索

文档翻译

学术文献翻译模型,支持多种主流文档格式。

立即体验