Atatürk University, Faculty of Dentistry, Prosthodontics Department, Erzurum, Turkey.
J Dent. 2012 Dec;40 Suppl 2:e41-6. doi: 10.1016/j.jdent.2012.07.014. Epub 2012 Jul 27.
The aim of this study was to evaluate the effects of staining solutions on the color stability of self-cure provisional resin materials.
The specimens were prepared for each of three auto-polymerized bis-acryl resin and auto-polymerized methyl methacrylate provisional resin material. The baseline color values were measured with a colorimeter according to the CIE L()a()b(*) color scale. After the first measurement (T(0)), specimens were placed in staining solutions (coffee, coca-cola, burn and distilled water for control group) and the other measurements were taken after 24h (T(1)), 1 week (T(2)) and 4 weeks (T(3)).
Data were analyze statistically by (a) repeated measures (ANOVA), (b) one and two way ANOVA, and (c) Tukey HSD multiple comparison tests. At the 24h immersion period, the post hoc analysis indicated that AccessCrown-coffee revealed the highest ΔE() values (4.4). At the second immersion period (1 week), Structur2 SC-coffee had the highest ΔE() values compared with other materials (5.4).
The degrees of discoloration were increased with immersion time. The methylmethacrylate resin was more resistant to discoloration than bis-acryl resins. After immersion for 30 days, the coffee solution resulted in unacceptable discoloration for all the tested materials.
本研究旨在评估染色溶液对自固化临时树脂材料颜色稳定性的影响。
为三种自聚合双丙烯酸树脂和自聚合甲基丙烯酸甲酯临时树脂材料的每个样本制备标本。根据 CIE L()a()b(*)颜色标度,用色度计测量基线颜色值。第一次测量(T(0))后,将标本放置在染色溶液中(咖啡、可口可乐、烧伤和蒸馏水作为对照组),并在 24 小时(T(1))、1 周(T(2))和 4 周(T(3))后进行其他测量。
数据通过(a)重复测量(ANOVA)、(b)单向和双向 ANOVA 以及(c)Tukey HSD 多重比较检验进行统计分析。在 24 小时浸泡期,事后分析表明 AccessCrown-咖啡显示出最高的 ΔE()值(4.4)。在第二次浸泡期(1 周),与其他材料相比,Structur2 SC-咖啡的 ΔE()值最高(5.4)。
随着浸泡时间的增加,变色程度增加。甲基丙烯酸甲酯树脂比双丙烯酸树脂更耐变色。浸泡 30 天后,所有测试材料的咖啡溶液都导致不可接受的变色。