School of Chemical Engineering, College of Engineering and Physical Sciences, University of Birmingham, Edgbaston, Birmingham, UK.
Biotechnol Bioeng. 2013 Jun;110(6):1714-25. doi: 10.1002/bit.24842. Epub 2013 Feb 22.
Cerium (IV) initiated "graft-from" polymerization reactions were employed to convert M-PVA magnetic particles into polyacrylic acid-fimbriated magnetic cation exchange supports displaying ultra-high binding capacity for basic target proteins. The modifications, which were performed at 25 mg and 2.5 g scales, delivered maximum binding capacities (Qmax ) for hen egg white lysozyme in excess of 320 mg g(-1) , combined with sub-micromolar dissociation constants (0.45-0.69 µm) and "tightness of binding" values greater than 49 L g(-1) . Two batches of polyacrylic acid-fimbriated magnetic cation exchangers were combined to form a 5 g pooled batch exhibiting Qmax values for lysozyme, lactoferrin, and lactoperoxidase of 404, 585, and 685 mg g(-1) , respectively. These magnetic cation exchangers were subsequently employed together with a newly designed "rotor-stator" type HGMF rig, in five sequential cycles of recovery of lactoferrin and lactoperoxidase from 2 L batches of a crude sweet bovine whey feedstock. Lactoferrin purification performance was observed to remain relatively constant from one HGMF cycle to the next over the five operating cycles, with yields between 40% and 49% combined with purification and concentration factors of 37- to 46-fold and 1.3- to 1.6-fold, respectively. The far superior multi-cycle HGMF performance seen here compared to that observed in our earlier studies can be directly attributed to the combined use of improved high capacity adsorbents and superior particle resuspension afforded by the new "rotor-stator" HGMS design.
铈(IV)引发的“从接枝”聚合反应被用于将 M-PVA 磁性颗粒转化为聚丙烯酸纤维状磁性阳离子交换载体,对碱性靶蛋白表现出超高的结合容量。在 25mg 和 2.5g 规模下进行的修饰,使鸡卵清白溶菌酶的最大结合容量(Qmax)超过 320mg/g,同时具有亚毫摩尔的离解常数(0.45-0.69μm)和大于 49L/g 的“结合紧密度”值。两批聚丙烯酸纤维状磁性阳离子交换剂被组合成一个 5g 的合并批次,对溶菌酶、乳铁蛋白和乳过氧化物酶的 Qmax 值分别为 404、585 和 685mg/g。这些磁性阳离子交换剂随后与新设计的“转子-定子”型 HGMF 装置一起,在从 2L 批次的粗甜牛初乳原料中连续五次回收乳铁蛋白和乳过氧化物酶的过程中使用。在五个操作循环中,从一个 HGMF 循环到下一个循环,乳铁蛋白的纯化性能观察到相对稳定,产率在 40%至 49%之间,纯化和浓缩因子分别为 37 至 46 倍和 1.3 至 1.6 倍。与我们早期研究中观察到的相比,这里看到的多循环 HGMF 性能的显著提高可以直接归因于改进的高容量吸附剂的联合使用和新的“转子-定子”HGMS 设计提供的优异的颗粒悬浮能力。