Hapa Onur, Akşahin Ertuğrul, Erduran Mehmet, Davul Serkan, Havitçioğlu Hasan, LaPrade Robert F, Bozdağ Ergun, Sünbüloğlu Emin
Department of Orthopedics and Traumatology, Dokuz Eylül University, İzmir, Turkey.
Knee. 2013 Dec;20(6):577-80. doi: 10.1016/j.knee.2012.11.010. Epub 2013 Jan 20.
Comparison of the mechanical characteristics of meniscal repair fixation using horizontal sutures and six different sutures under submaximal cyclic and load to failure test conditions may aid physicians in selecting a suture type.
A 2-cm long anteroposterior vertical longitudinal incision was created in six groups of bovine medial menisci. Lesions were repaired using a No. 2 suture either composed of polyester or polyester and ultra high-molecular weight polyethylene (UHMWPE), or UHMWPE and polydioxanone or pure UHMWPE. Endpoints included ultimate failure load (N), pull-out stiffness (N/mm), pull-out displacement (mm), cyclic displacement (mm) after 100cycles, after 500cycles, and mode of failure.
Polyester suture had lower ultimate load than all groups except the suture composed of polyester and UHMWPE (P<.05). Pure UHMWPE suture had higher ultimate failure load than sutures composed of either polyester or polyester plus UHMWPE (P<.05). Predominant failure mode was suture cutting through the meniscus for the groups except for polyester suture which failed by suture rupture.
Under cyclic loading conditions in bovine meniscus, braided polyester suture fixation provided lower initial fixation strength than fixation with various high strength sutures composed of pure UHMWPE or a combination of absorbable monofilament polydioxanone and UHMWPE, except for combination of polyester and UHMWPE sutures.
Present study does not support the usage of the braided polyester sutures instead of high strength sutures composed either partially or totally of ultra-high molecular weight polyethylene for the horizontal suture configuration of meniscus repair.
在次最大循环和破坏载荷试验条件下,比较使用水平缝线和六种不同缝线进行半月板修复固定的力学特性,可能有助于医生选择缝线类型。
在六组牛内侧半月板上制作一个2厘米长的前后垂直纵向切口。使用由聚酯或聚酯与超高分子量聚乙烯(UHMWPE)组成的2号缝线,或UHMWPE与聚二氧六环酮或纯UHMWPE修复损伤。观察指标包括极限破坏载荷(N)、拔出刚度(N/mm)、拔出位移(mm)、100次循环后、500次循环后的循环位移(mm)以及破坏模式。
聚酯缝线的极限载荷低于除聚酯与UHMWPE组成的缝线外的所有组(P<0.05)。纯UHMWPE缝线的极限破坏载荷高于由聚酯或聚酯加UHMWPE组成的缝线(P<0.05)。除聚酯缝线因缝线断裂失败外,其他组的主要破坏模式是缝线穿过半月板。
在牛半月板的循环加载条件下,编织聚酯缝线固定提供的初始固定强度低于由纯UHMWPE或可吸收单丝聚二氧六环酮与UHMWPE组合而成的各种高强度缝线固定,聚酯与UHMWPE缝线组合除外。
本研究不支持在半月板修复的水平缝线构型中使用编织聚酯缝线替代部分或全部由超高分子量聚乙烯组成的高强度缝线。